1. State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, Liaoning, China 2. Technical Centre of Hunan Valin Lianyuan Iron and Steel Co., Ltd., Loudi 417000, Hunan, China
Abstract:The production process of hot rolled dual phase (DP) steels with ultra fast cooling was investigated. The design rule of air cooling temperature/time, coiling temperature and rolling speed was introduced under stepped cooling mode. The reference values of each parameter was obtained using simulation calculation and based on the phase transformation theory. This process was applied on site and DP steel obtains the good properties with tensile strength of 700MPa.