Source and formation mechanism of inclusions in FeSiB amorphous ribbon
LI Bai-song1,2, CHEN Wen-zhi2, YAO Shu-fang2, ZHAO Yu-lin2
1. Central Iron and Steel Research Institute, China Iron and Steel Research Institute Group, Beijing 100081, China; 2. Advanced Technology and Materials Co., Ltd., China Iron and Steel Research Institute Group, Beijing 100081, China
Abstract:In order to formulate a reasonable inclusion control process to improve the quality and magnetic properties of FeSiB amorphous ribbon, the source and the formation mechanism of inclusions were analyzed. The results show that the spherical and elliptical inclusions consisted of Al2O3 and SiO2 mainly come from the industrial pure iron. During the next smelting process, ellipsoidal inclusions of 20-30 μm in the pure iron were removed by floatation, while spherical inclusions of 1-3 μm combined with the deoxidized products and form aluminum silicate inclusions and aluminum calcium silicate inclusions in FeSiB master alloy. Some of these inclusions accumulated in the inner wall of the nozzle during the spraying process, while the other parts of inclusions flowed out of the nozzle and remained in the FeSiB amorphous ribbon.
李百松, 陈文智, 姚书芳, 赵玉林. FeSiB非晶薄带中夹杂物的来源及形成机理[J]. 钢铁, 2020, 55(1): 27-33.
LI Bai-song, CHEN Wen-zhi, YAO Shu-fang, ZHAO Yu-lin. Source and formation mechanism of inclusions in FeSiB amorphous ribbon. Iron and Steel, 2020, 55(1): 27-33.
[1] LIU Y H,WANG G,WANG R J,et a1. Super plastic bulk metallic glasses at room temperature[J]. Science,2007,315(5817):1385. [2] ZHAO D G,GUO P M,ZHAO P. Activity model of Fe78-Si9B13 ternary metallic melts[J]. Journal of Iron and Steel Reseach,International, 2011,18(6):16. [3] QIAO J W,JIA H L,LIAW P K. Metallic glass matrix composites[J]. Materials Science and Engineering R:Reports,2016,100:1. [4] 杜毓铣,张传历,马鸿良,等. 非晶宽带的工艺性缺陷[J]. 钢铁,1982,17(7):39.(DU Yu-xian,ZHANG Chuan-li,MA Hong-liang,et al. Technological defects of broad amorphous ribbons[J]. Iron and Steel,1982,17(7):39.) [5] 肖阳,张磊,杜帅龙,等. Finemet型铁基非晶带材异常缺陷分析[J]. 金属功能材料,2017,24(6):5.(XIAO Yang,ZHANG Lei,DU Shuai-long,et al. The defect analysis of Finemet type iron-based amorphous ribbons[J]. Metallic Functional Materials,2017,24(6):5.) [6] 王建,周少雄,颜慧成,等. Fe-Si-B非晶合金制备过程中的水口结瘤分析[J]. 钢铁研究学报,2013,25(7):111.(WANG Jian,ZHOU Shao-xiong,YAN Hui-cheng,et al. Analysis on nozzle clogging in casting of Fe-Si-B amorphous alloy[J]. Journal of Iron and Steel Research,2013,25(7):111.) [7] 李百松,陈文智,王建,等. Fe-Si-B合金中非金属夹杂物的热力学分析[J]. 钢铁研究学报,2016,28(9):50.(LI Bai-song,CHEN Wen-zhi,WANG Jian,et al. Thermodynamic analysis on non-metallic inclusions in Fe-Si-B alloy[J]. Journal of Iron and Steel Research,2016,28(9):50.) [8] 彭其春, 邱雷, 邹健, 等. 无取向硅钢W800生产过程中夹杂物演变规律[J]. 钢铁, 2015, 50(8): 34.(PENG Qi-chun,QIU Lei,ZOU Jian,et al. Evolution of inclusions in non-oriented silicon steel W800 during production process[J]. Iron and Steel,2015,50(8):34.) [9] 李牧明, 于会香, 潘明, 等. 精炼渣对高锰钢中非金属夹杂物的影响[J]. 钢铁, 2019, 54(6): 37.(LI Mu-ming,YU Hui-xiang,PAN Ming,et al. Effect of refining slag on non-metallic inclusions in high manganese steel[J]. Iron and Steel,2019,54(6):37.) [10] 刘延强, 张鹏, 何文远, 等. X65管线钢全流程夹杂物转变规律及控制[J]. 钢铁, 2018, 53(12): 44.(LIU Yan-qiang,ZHANG Peng,HE Wen-yuan,et al. Transformation behavior and control of inclusions in X65 pipelinesteel during whole process[J]. Iron and Steel,2018,53(12):44.) [11] 邓志银, 朱苗勇. 合金钢中MnO/FeO大型夹杂物来源分析[J]. 钢铁, 2018, 53(2): 27.(DENG Zhi-yin,ZHU Miao-yong. Transformation behavior and control of inclusions in X65 pipelinesteel during whole process[J]. Iron and Steel,2018,53(2):27.) [12] 张先棹. 冶金传输原理[M]. 北京:冶金工业出版社,1988.(ZHANG Xian-zhao. Metallurgy Transport Principle[M]. Beijing:Metallurgical Industry Press,1988.) [13] LI C D,TIAN X L,CHEN X C,et a1. Viscosity measurements of Fe-Si-B-Cu-Nb-C metallic glass melts by an oscillating crucible method[J]. Chinese Physics Letters,2003,20(3):395. [14] 黄希祜. 钢铁冶金原理[M]. 北京:冶金工业出版社,2002.(HUANG Xi-hu. Principles of Iron and Steel Metallurgy[M]. Beijing:Metallurgical Industry Press,2002.)