Effect of heat treatment process on microstructure and property of 2Cr12NiMo1W1V steel for steam blade
WANG Li-wei1, GONG Zhi-hua2, YANG Gang2, ZHAO Ji-qing2
1. Jiangyou Changcheng Special Steel Co., Ltd., Pangang Group, Jiangyou 621700, Sichuan, China; 2. Institute of Special Steels, Central Iron and Steel Research Institute, Beijing 100081, China
Abstract:In order to solve the problem of low creep fracture time of 2Cr12NiMo1W1V steel,the microstructure,room temperature mechanical properties and short-term creep fracture strength of 2Cr12NiMo1W1V martensitic heat-resistant steel for ultra-supercritical blades under different quenching and tempering processes were studied by means of OM,SEM and TEM. The results show that the tensile strength and impact absorbing energy increase and the yield strength and hardness decrease with the increase of quenching temperature. The optimized heat treatment process of 2Cr12NiMo1W1V is quenching at 1 038 ℃ and tempering at 675 ℃. The strength,toughness and durability of the alloy have good match. The microstructure analysis shows that with the increase of quenching temperature,the carbide of M23C6with big size in the alloy is more solid solution in the matrix,and result in a large number of fine M23C6 phases are precipitated during tempering. Which reduces the crack origin in the short-term creep test process,at the same time,the dislocation movement was hindered. Thus the ability of the alloy resist high-temperature deformation increased,and the creep fracture property of the alloy is improved.
王利伟, 龚志华, 杨钢, 赵吉庆. 热处理工艺对2Cr12NiMo1W1V叶片钢组织和性能的影响[J]. 钢铁, 2020, 55(7): 100-105.
WANG Li-wei, GONG Zhi-hua, YANG Gang, ZHAO Ji-qing. Effect of heat treatment process on microstructure and property of 2Cr12NiMo1W1V steel for steam blade[J]. Iron and Steel, 2020, 55(7): 100-105.
[1] 杨钢,王立民,程世长,等. 蒸汽轮机用叶片钢的研究进展[J]. 特钢技术,2009,15(3):1.(YANG Gang,WANG Li-min,CHENG Shi-chang,et al. The study progress for the blade steels for the steam turbine[J]. Special Steel Technology,2009,15(3):1.) [2] 刘新权,杨钢,杨沐鑫. 1Cr11Co3W3MoVNbNB铁素体叶片钢620 ℃时效M23C6和MX第二相的析出行为[J]. 钢铁研究学报,2012,28(5):53.(LIU Xin-quan,YANG Gang,YANG Mu-xin. Precipitation behavior of M23C6 and MX second phase in 1Cr11Co3W3MoVNbNB ferrite-blade-steel at 620 ℃ aging treatment[J]. Journal of Iron and Steel Research,2012,28(5):53.) [3] 龚志华,何禛,包汉生,等. 2Cr12NiMo1W1V超临界汽轮机叶片用耐热钢的热变形行为[J]. 钢铁,2019,54(3):63. (GONG Zhi-hua,HE Zhen,BAO Han-sheng,et al. Hot deformation behavior of 2Cr12NiMo1W1V heat resistant steel used for supercritical steam turbine blades[J]. Iron and Steel,2019,54(3):63.) [4] 龚志华,杨钢,定巍,等. 热处理工艺对1Cr11Co3W3MoVN-bNB钢析出相及性能的影响[J]. 钢铁研究学报,2018,30(4):315.(GONG Zhi-hua,YANG Gang,DING Wei,et al. Effect of heat treatment process on precipitation behavior and mechanical properties of 1Cr11Co3W3MoVNbNB[J].Journal of Iron and Steel Research,2018,30(4):315.) [5] Viswanathan R,Henry J F,Tanzosh J,et al. U.S. Program on materials technology for ultra-supercritical coal power plants[J]. Journal of Materials Engineering and Performance,2005,14(3):281. [6] Bugge J,Kjær S,Blum R. High-efficiency coal-fired power plants development and perspectives[J]. Energy,2006,31(10):1437. [7] 龚志华,杨钢,定巍. 热处理工艺对1Cr11Co3W3MoVNbNB钢析出相及性能的影响[J]. 钢铁研究学报,2018,30(4):315. (GONG Zhi-hua,YANG Gang,DING Wei. Effect of heat treatment process on precipitation behavior and mechanical properties of 1Cr11Co3W3MoVNbNB[J]. Journal of Iron and Steel Research,2018,30(4):315.) [8] 汪开忠,郝震宇,胡芳忠,等. 高压锅炉管用P91钢热处理工艺优化[J]. 中国冶金,2018,28(5):58.(WANG Kai-zhong,HAO Zhen-yu,HU Fang-zhong,et al. Optimization on heat-treatment process of P91 steel for high pressure boiler tube[J]. China Metallurgy,2018,28(5):58.) [9] 丁建生,刘蔺勋. 热处理对超超临界材料KT5331ASO组织和性能的影响[J]. 热加工工艺,2010,39(8):166.(DING Jian-sheng,LIU Lin-xun. The influence of heat treatment on the structure and properties of KT5331ASO for the ultra-super critical steam turbine[J]. Hot Working Technology,2010,39(8):166.) [10] 梁娟. 600-650 ℃超超临界汽轮机转子材料的高温力学性能分析[J]. 上海电机学院学报,2012,15(2):133.(LIANG Juan. High temperature mechanical property analysis for the material used for the ultra-super critical steam turbine rotor working at 600-650 ℃[J]. Journal of Shanghai Dianji University,2012,15(2):133.)