Stamping Cracking Mechanism of High Strength Beam Steel of 750MPa Level |
YU Yang1,MENG Xian-tang1,WANG Lin1,WANG Chang1,LI Fei1,LI Rui-heng2 |
1. Shougang Research Institute of Technology, Sheet Metal Research Institute, Beijing 100043, China 2. Shougang Qian’an Steel Company, Technology and Quality Division, Qian’an 064404, Hebei, China |
|
|
Abstract The stamping cracking defect is the main problem for the utility of high strength beam steel with the strength exceeding 700MPa. Controlling the inclusions and center segregation and grinding the shear plane can reduce the probability of stamping cracking. The paper was mainly focused on hot rolling process to investigate the cause and mechanism leading to stamping cracking. The microstructure, mechanical properties, heating and rough rolling temperature system, finishing rolling and coiling temperature system, finishing rolling speed, as well as the influence of hot charging system, were all comparatively analyzed, considering the difference between the normal strip and stamping cracking strip of 750 MPa level beam steel. And some beneficial experiences were provided for production of this kind of steel. The results show that ensuring fine rolling speed is the important way to low the probability of stamping cracking defect.
|
Received: 06 May 2013
Published: 28 April 2014
|
|
|
|
[1] |
东方.700MPa高强钢在商用车领域将大有可为[J].设备与材料,2012,(8):86-87
|
[1] |
东方.700MPa高强钢在商用车领域将大有可为[J].设备与材料,2012,(8):86-87
|
[2] |
赵培林,路峰,王建景,等.700MPa级超高强度汽车大梁用钢研究与开发[J].轧钢,2011,28(2):12-16
|
[2] |
赵培林,路峰,王建景,等.700MPa级超高强度汽车大梁用钢研究与开发[J].轧钢,2011,28(2):12-16
|
[3] |
王晓南,杜林秀,张海仑,等.780MPa级重载汽车用大梁钢的工业试制[J].钢铁研究学报,2011,23(5):45-49
|
[3] |
王晓南,杜林秀,张海仑,等.780MPa级重载汽车用大梁钢的工业试制[J].钢铁研究学报,2011,23(5):45-49
|
[4] |
韩斌,时晓光,董毅,等.超高强汽车大梁钢700L的开发研制[J].鞍钢技术,2012,(5):10-13
|
[4] |
韩斌,时晓光,董毅,等.超高强汽车大梁钢700L的开发研制[J].鞍钢技术,2012,(5):10-13
|
[5] |
赵培林,孙新军,雍岐龙,等.超高强度热轧钢板冷冲压开裂原因及分析[J].金属热处理,2012,37(7):122-126
|
[5] |
赵培林,孙新军,雍岐龙,等.超高强度热轧钢板冷冲压开裂原因及分析[J].金属热处理,2012,37(7):122-126
|
[6] |
郑东升,朱伏先,李艳梅,等.控轧控冷工艺对汽车大梁板组织及冷弯性能的影响[J].中国冶金,2009,19(5):17-20
|
[6] |
郑东升,朱伏先,李艳梅,等.控轧控冷工艺对汽车大梁板组织及冷弯性能的影响[J].中国冶金,2009,19(5):17-20
|
[7] |
赵楠,穆海玲,周丽萍,等.BM510汽车大梁钢冷弯开裂原因分析机[J].械工程材料,2008,32(11):72-74
|
[7] |
赵楠,穆海玲,周丽萍,等.BM510汽车大梁钢冷弯开裂原因分析机[J].械工程材料,2008,32(11):72-74
|
[8] |
方圆,阳代军,张宏艳,等.汽车大梁钢510L冲压开裂原因分析[J].热加工工艺,2012,41(3):169-172
|
[8] |
方圆,阳代军,张宏艳,等.汽车大梁钢510L冲压开裂原因分析[J].热加工工艺,2012,41(3):169-172
|
[9] |
张宜,胡学文,万文红.屈服强度700MPa级超高强度大梁钢冲压开裂原因的分析[J].安徽冶金,2009,(3):33-35
|
[9] |
张宜,胡学文,万文红.屈服强度700MPa级超高强度大梁钢冲压开裂原因的分析[J].安徽冶金,2009,(3):33-35
|
[1] |
YU Hui-xiang, PAN Ming, YANG De-xin. Behavior of inclusions in ultra-low carbon IF steel during deoxidation and alloying process[J]. Iron and Steel, 2020, 55(6): 46-53. |
[2] |
ZHAO Yun-peng, YU Chao, XIAO Hong, WU Zong-he, XU Peng-peng, XIE Hong-biao. Effect of pure iron interlayer on mechanical properties of hot rolled stainless steel clad plate[J]. Iron and Steel, 2020, 55(5): 73-79. |
[3] |
SUN Ming-han, ZHENG Yi, QU Chun-tao, JIN Shi-zhe, XU Zhi-qiang, DU Feng-shan. Numerical simulation of temperature field in ultra-fast cooling process of hot rolled plate[J]. Iron and Steel, 2020, 55(3): 50-57. |
[4] |
CAI Zhen, LIANG Wen, WANG Shui-ze, LIU Yong-qian. Discussion about practice and process of ferrite rolling in Ti-IF steel[J]. PHYSICS EXAMINATION AND TESTING, 2020, 38(3): 7-. |
[5] |
ZHOU Cong-rui, CHEN Xiao-long, ZHOU Ming-ke,FAN Lei, MEI Peng, BAO Si-qian. Cause analysis of surface blackening of SPHC hot rolled strip after pickling[J]. PHYSICS EXAMINATION AND TESTING, 2020, 38(3): 41-. |
[6] |
JIANG Da-jun. Influence of fuel structure on sintering character and comprehensive effect[J]. Iron and Steel, 2020, 55(2): 31-41. |
|
|
|
|