Effects of Thermo-Magnetic Treatment on Microstructure and Mechanical Properties of Rolling-Bearing Steel |
|
|
Abstract The influence of thermo-magnetic treatment of rolling-bearing steel on some its metallurgical and mechanical properties was investigated. The heating and/or cooling processes of the sample occurred in a magnetic field having certain intensities. The XRD patterns of rolling-bearing steel sample exhibited a beneficial effect of the magnetic field on the structure, phase transformation and tension state. It was found an increased reliability of rolling tribomodel made from thermo-magnetic treated steel when it was subjected to the fatigue tests.
|
Received: 29 September 2009
|
|
|
|
[1] |
Hai-yan Tang*,Yong Wang,Guang-hui Wu,Peng Lan,Jia-quan Zhang. Inclusion evolution in 50CrVA spring steel by optimization of refining slag[J]. Chinese Journal of Iron and Steel, 2017, 24(9): 879-887. |
[2] |
H. Gonzalez,J.A. Ramos-Banderas,E. Torres-Alonso,G. Solorio-Diaz,C.A. Hern��ndez-Bocanegra,. Multiphase modeling of fluid dynamic in ladle steel operations under non-isothermal conditions[J]. Chinese Journal of Iron and Steel, 2017, 24(9): 888-900. |
[3] |
Zong-ye Ding,Di Zhang,Qiao-dan Hu,,*,Long Zeng,Jian-guo Li,. Constitutive analysis and optimization on hot working parameters of as-cast high Cr ultra-super-critical rotor steel with columnar grains[J]. Chinese Journal of Iron and Steel, 2017, 24(9): 916-924. |
[4] |
Hao Li,Yan-chong Yu,,Xiang Ren,Shao-hua Zhang,She-bin Wang,,*. Evolution of Al2O3 inclusions by cerium treatment in low carbon high manganese steel[J]. Chinese Journal of Iron and Steel, 2017, 24(9): 925-934. |
[5] |
Yu-cheng Lei,,*,Xiao-kai Guo,Hong-xia Chang,Tian-qing Li,,Qiang Zhu,Gang Chen, Long-ren Xiao. Cavitation erosion behavior of CLAM steel weld joint in liquid lead-bismuth eutectic alloy[J]. Chinese Journal of Iron and Steel, 2017, 24(9): 935-942. |
[6] |
Zhen Cao,Shu-qi Wang*,Ke-zhi Huang,Bo Zhang,Guo-hong Wen,Qiu-yang Zhang,Lan Wang. Effect of artificial tribological layer on sliding wear behavior of H13 steel[J]. Chinese Journal of Iron and Steel, 2017, 24(9): 943-949. |
|
|
|
|