Evolution of Surface Transversal Crack in Intermediate Slabs during Hot Rolling Deformation |
Yan-zhao LUO,Jiong-ming ZHANG,Qiang LIU,Mao-kang LI,Yi-tong HAN,Yi-fei CAO |
School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China |
|
|
Abstract In the continuous casting of steels, surface transversal cracks are often found. These defects may severely influence the final quality of the products. The evolution of transversal V-shaped cracks with different depth on the surface of a continuously cast steel slab during hot rolling was studied. The artificial V-shaped cracks were made on the surface. The rolling process parameters from an industrial rolling mill have been used as a reference. The specimens of rolled workpiece in intermediate slabs were obtained after different rolling passes. The morphology of surface crack and microstructure evolution in the rolling process were investigated by optical microscopy. The results show that the depth of surface transversal crack gradually decreased with the increase of rolling passes. The grain size of ferrite and pearlite on the sample surface also gradually reduced. The microstructures around cracks with the different depth are almost identical, without direct correlation with the initial crack depth.
|
Received: 26 November 2012
Published: 15 April 2014
|
Corresponding Authors:
Yanzhao Luo
E-mail: luoyanzhao@hotmail.com
|
|
|
|
[1] |
Ying Ci,*,Zhan-zhan Zhang. Simulation study on heat-affected zone of high-strain X80 pipeline steel[J]. Chinese Journal of Iron and Steel, 2017, 24(9): 966-973. |
[2] |
Xiao-li Zhao,,Yong-jian Zhang,Cheng-wei Shao,Wei-jun Hui,Han Dong. Thermal stability of retained austenite and mechanical properties of medium-Mn steel during tempering treatment[J]. Chinese Journal of Iron and Steel, 2017, 24(8): 830-837. |
[3] |
Hang-wei Zhou,,Hui-qun Liu,,Dan-qing Yi,,Yu Xiao,,Xiao-long Zhao,Jian Wang,Qi Gao. Effect of �� phase on fatigue crack growth of Ti-6242 alloy[J]. Chinese Journal of Iron and Steel, 2017, 24(8): 811-822. |
[4] |
Reng-chong Xu,,Yan-lin He,,Hu Jiang,,Hua Wang,,Na-qiong Zhu,,Xiao-gang Lu,, Lin Li,. Microstructures and mechanical properties of ferrite-based lightweight steel with different compositions[J]. Chinese Journal of Iron and Steel, 2017, 24(7): 737-742. |
[5] |
Wei-jun Hui,*,Na Xiao,Xiao-li Zhao,Yong-jian Zhang,Yu-feng Wu. Effect of vanadium on dynamic continuous cooling transformation behavior of medium-carbon forging steels[J]. Chinese Journal of Iron and Steel, 2017, 24(6): 641-648. |
[6] |
Yong-xing Jiao,Jian-sheng Liu*,Xing-wang Duan,Xiao-hua Zheng,Wen-wu He. Prediction of critical forging penetration efficiency for 06Cr19Ni9NbN steel by dynamic recrystallization[J]. Chinese Journal of Iron and Steel, 2017, 24(6): 649-653. |
|
|
|
|