Effect of MgO on Oxidation Process of Fe3O4 in Pellets |
Qiang-jian GAO1,Yan-song SHEN2,Xin JIANG1,Hai-yan ZHENG1,Feng-man SHEN1,Chang-sheng LIU1 |
1. School of Metallurgy, Northeastern University, Shenyang 110819, Liaoning, China 2. School of Chemical Engineering, University of New South Wales, New South Wales 2052, Australia |
|
|
Abstract Induration process of oxidized pellets involves the oxidation of Fe3O4 and re-crystallization of Fe2O3. The oxidation process of Fe3O4 is significant for pellets to obtain better ambient strength. Thus, the effect of MgO on oxidation process of Fe3O4 was investigated. The unreacted core model was applied to analyze the oxidizing induration process of pellets. The experimental results show that MgO plays a negative role in the oxidation process of Fe3O4. The oxidation rate of Fe3O4 in MgO-fluxed pellets (95.0% Fe3O4+5.0% MgO) is slower than that in standard acid pellets (100% Fe3O4). The relation between oxidation ratio of Fe3O4 and time was calculated based on the unreacted core model for both MgO-fluxed pellets and standard acid pellets. According to verification experiments, the values calculated by model coincide well with the experimental values. Therefore, the unreacted core model could be applied to describe the oxidizing induration process of pellets.
|
Received: 16 October 2015
Published: 18 October 2016
|
Fund:National Science Foundation of China |
Corresponding Authors:
Qiang-Jian GAO
E-mail: gaoqiangjian@163.com
|
|
|
|
[1] |
Yu-cheng Lei,,*,Xiao-kai Guo,Hong-xia Chang,Tian-qing Li,,Qiang Zhu,Gang Chen, Long-ren Xiao. Cavitation erosion behavior of CLAM steel weld joint in liquid lead-bismuth eutectic alloy[J]. Chinese Journal of Iron and Steel, 2017, 24(9): 935-942. |
[2] |
Ying-yi Zhang,Wei Lv,Xue-wei Lv,Chen-guang Bai,Ke-xi Han,Bing Song. Oxidation kinetics of ilmenite concentrate by non-isothermal thermogravimetric analysis[J]. Chinese Journal of Iron and Steel, 2017, 24(7): 678-684. |
[3] |
Rui Wang,Yan-ping Bao,*,Yi-hong Li,Tai-quan Li,Di Chen. Effect of slag composition on steel cleanliness in interstitial-free steel[J]. Chinese Journal of Iron and Steel, 2017, 24(6): 579-585. |
[4] |
Hong-huan Mao,Xing Qi,Jing Cao,Li-cong An,Yi-tao Yang*. Effect of Si on high temperature oxidation of 30Cr13 stainless steel[J]. Chinese Journal of Iron and Steel, 2017, 24(5): 561-566. |
[5] |
Yong-jiang Huang,,,*,Peng Xue,Xiang Cheng,Ya-ming Wang,Fu-yang Cao,**, Zhi-liang Ning, Jian-fei Sun,. Plasticity improvement of a Zr-based bulk metallic glass by micro-arc oxidation[J]. Chinese Journal of Iron and Steel, 2017, 24(4): 416-420. |
[6] |
Shi-lu Zhao,*,Zhen Zhang,Jun Zhang,Jian-ming Wang,Zheng-gui Zhang,Shuang-hong Wang. High temperature oxidation resistance of CrN/(Ti,Al,Zr,Cr)N bilayer films deposited by multi-arc ion plating[J]. Chinese Journal of Iron and Steel, 2017, 24(3): 343-349. |
|
|
|
|