Oxidation Behavior of Fe-based Amorphous Ribbons |
Shu-lan ZHANG,He-ping LIU,Xiao-tong FU |
Central Iron and Steel Research Institute, Beijing 100081, China |
|
|
Abstract The oxidation behavior of Fe-based amorphous ribbons was tested by annealing at 380 �� in air for different time with heat treatment furnace and analyzed by X-ray photoelectron spectroscopy (XPS) and scanning electron microscopy (SEM). The mechanism of oxides formation of the amorphous ribbons was discussed in detail. The results showed that the oxides were mostly B2O3, SiO2 and Fe2O3 or FeO. With the increase of annealing time and holding temperature, the fraction of the oxides on the ribbon surface increased and the size of the oxides became larger due to the generation of new oxides and the coalescence of small oxides. The oxides have different shapes, such as round, rod and needle-shaped. Experimental results also showed that the oxides nucleated at fish scale, air pocket and impurities in priority, and the growth of the oxides was controlled by the diffusion of atoms. With the increase of the distance to the ribbon surface, the oxygen concentration decreased dramatically. Due to the low binding energy of B2O3 and the large diffusion coefficient of B atom, the B element was oxidized firstly compared with other elements. Moreover, the oxidation depths of the B2O3 and SiO2 were larger than that of Fe2O3.
|
Received: 22 February 2016
Published: 04 November 2016
|
Fund:Natural Science Foundation of China |
Corresponding Authors:
shulan
E-mail: shlzhang_cisri@sina.com
|
|
|
|
[1] |
Yu-cheng Lei,,*,Xiao-kai Guo,Hong-xia Chang,Tian-qing Li,,Qiang Zhu,Gang Chen, Long-ren Xiao. Cavitation erosion behavior of CLAM steel weld joint in liquid lead-bismuth eutectic alloy[J]. Chinese Journal of Iron and Steel, 2017, 24(9): 935-942. |
[2] |
Ying-yi Zhang,Wei Lv,Xue-wei Lv,Chen-guang Bai,Ke-xi Han,Bing Song. Oxidation kinetics of ilmenite concentrate by non-isothermal thermogravimetric analysis[J]. Chinese Journal of Iron and Steel, 2017, 24(7): 678-684. |
[3] |
Rui Wang,Yan-ping Bao,*,Yi-hong Li,Tai-quan Li,Di Chen. Effect of slag composition on steel cleanliness in interstitial-free steel[J]. Chinese Journal of Iron and Steel, 2017, 24(6): 579-585. |
[4] |
Hong-huan Mao,Xing Qi,Jing Cao,Li-cong An,Yi-tao Yang*. Effect of Si on high temperature oxidation of 30Cr13 stainless steel[J]. Chinese Journal of Iron and Steel, 2017, 24(5): 561-566. |
[5] |
Yong-jiang Huang,,,*,Peng Xue,Xiang Cheng,Ya-ming Wang,Fu-yang Cao,**, Zhi-liang Ning, Jian-fei Sun,. Plasticity improvement of a Zr-based bulk metallic glass by micro-arc oxidation[J]. Chinese Journal of Iron and Steel, 2017, 24(4): 416-420. |
[6] |
Hui-hui Xiong,,*,Heng-hua Zhang,Hui-ning Zhang,Yang Zhou. Effects of alloying elements X (X=Zr, V, Cr, Mn, Mo, W, Nb, Y) on ferrite/TiC heterogeneous nucleation interface: first-principles study[J]. Chinese Journal of Iron and Steel, 2017, 24(3): 328-334. |
|
|
|
|