Initiation and propagation of localized corrosion induced by (Zr, Ti, Al)-Ox inclusions in low-alloy steels in marine environment |
Wen-zhui Wei1, Kai-ming Wu1, Jing Liu1, Lin Cheng1, Xian Zhang1 |
1 The State Key Laboratory of Refractories and Metallurgy, Hubei Province Key Laboratory of Systems Science in Metallurgical Process, Collaborative Innovation Center for Advanced Steels, Wuhan University of Science and Technology, Wuhan 430081, Hubei, China |
|
|
Abstract The effects of inclusions on localized corrosion of Zr–Ti deoxidized low-alloy steels in marine environment were investigated by various analytical techniques including scanning electron microscopy with X-ray microanalysis (SEM/ EDS), confocal Raman microscopy (CRM), and in situ scanning vibrating electrode technique (SVET). It was found that complex (Zr, Ti, Al)-Ox inclusions were responsible for the initiation of localized corrosion. Localized corrosion preferentially occurred at Fe matrix adjacent to these inclusions and formed micro-gaps. In the early stage of corrosion, catalytic-occluded cells and the diffusion of chloride ions played a major role in the propagation of corrosion, further accelerating the dissolution of Fe matrix and (Zr, Ti, Al)-Ox inclusions. Combining SVET and CRM results, it revealed that the maximum anodic current density in local area gradually decreased with prolonged exposure time, indicating that corrosion products covered the steel surface and lowered the propagation rate of corrosion. In the later stage of corrosion, the barrier effect of corrosion products played an important role in inhibiting localized corrosion.
|
|
|
|
|
Cite this article: |
Wen-zhui Wei,Kai-ming Wu,Jing Liu, et al. Initiation and propagation of localized corrosion induced by (Zr, Ti, Al)-Ox inclusions in low-alloy steels in marine environment[J]. Journal of Iron and Steel Research International, 2021, 28(4): 453-463.
|
|
|
|
[1] |
WANG Ping,GUANG Jianfeng,HOU Qingyu,GUO Aimin,HUANG Zhenyi. Formation and control of carbide in aged lowdensity untralow carbon steel[J]. JOURNAL OF IRON AND STEEL RESEARCH , 2021, 33(4): 336-344. |
[2] |
SUI Ya-fei, DENG Zhi-xun, ZHAO Ru, QI Jiang-hua. Inclusions in hot rolled pickling plate for automobile structure through CSP process[J]. Iron and Steel, 2021, 56(4): 44-51. |
[3] |
Jing‑jing Pei, Jin‑hu Wu, Wen‑qing Huo, Yu‑zhu Zhang, Hong‑wei Xing, Qian‑qian Ren. Structure characterization and grinding performance of gas-quenched steel slag abrasive[J]. JOURNAL OF IRON AND STEEL RESEARCH,INTERNATIONAL, 2021, 28(4): 383-390. |
[4] |
Chun‑chao Huang, Xiao‑jun Ning, Guang‑wei Wang, Jian‑liang Zhang, Zheng‑fu Peng, Hai‑peng Teng. Experimental research on semi-coke for blast furnace injection[J]. JOURNAL OF IRON AND STEEL RESEARCH,INTERNATIONAL, 2021, 28(4): 391-401. |
[5] |
Lei Cao, De-li Shang, Xin-gang Ai, Peng-liang Jin, Yuan-you Xiao, Guo-cheng Wang, Chun-wei Liu. Effect of trace Si on MgOAl2O3 inclusion in ultra-low-carbon steel[J]. JOURNAL OF IRON AND STEEL RESEARCH,INTERNATIONAL, 2021, 28(4): 402-412. |
[6] |
Zhen Ning, Wei Yu, Hong-qiang Liu, Qing-wu Cai. Effect of reduction pretreatment process on evolution of microporosity in 42CrMo billet[J]. JOURNAL OF IRON AND STEEL RESEARCH,INTERNATIONAL, 2021, 28(4): 413-423. |
|
|
|
|