Technical Study and Application of Split Roller Cooling Water Sealing of Caster in Shouqin |
LI Song-shan,DUAN Xue-liang,FAN Xing-chen,LI Xue-rong,SUN Bo |
Shouqin Metal Material Company, Qinhuangdao 066000,Hebei, China |
|
|
Abstract Leaking between the three split rollers of caster segment for the non-entire shaft roller has a serious influence on the surface quality of the slab and the costs of segment maintenance. In this study, the characteristics and reasons of leakage points section of the roller were analyzed, and the key point was obtained which is that how to ensure the synchronization of three split rollers and nonrigid connection between rollers. According to the analysis, the slider with a cross shaft coupling was confirmed. Practice proved that the scheme can perfect the solution of the three split rollers leaking problem, and greatly prolong the roller life, and improve the surface quality of slab.
|
Received: 29 November 2012
Published: 28 May 2013
|
|
|
|
[1] |
WANG En-rui, CHEN Zi-gang, LIU Feng-lin, LIU Tian-wu, ZHANG Ming. Oxide scale structure of hot rolled structural steel and its effect on pickling quality[J]. Iron and Steel, 2022, 57(3): 71-78. |
[2] |
ZHANG Fu-jun, YANG Shu-feng, WANG Yong, HUANG Cheng-yong, LI Jing-sheng, YANG Jing-bo. Surface quality control of fine blanking steel slab[J]. CONTINUOUS CASTING, 2022, 41(2): 20-24. |
[3] |
ZENG Bing,LIU Rongfeng,YUAN Jie,LIANG Xiaodong. Hazard analysis of copper metal pollution on surface of steel pipe[J]. PHYSICS EXAMINATION AND TESTING, 2021, 39(6): 50-. |
[4] |
SUN Jian-liang, SUN Meng-qian, GUO He-song, JI Jiang, XU Li-pu, PENG Yan. Comprehensive prediction of surface quality of hot-rolled strip with multiple and single defects[J]. Iron and Steel, 2021, 56(1): 51-58. |
[5] |
WEI Jun-you, ZHAO Wen-bo, CHEN Li, HU Peng, LIU Chong-lin, WAN Xiu-juan. Causes analysis of surface upwarping defects on hot rolled strip[J]. CONTINUOUS CASTING, 2020, 39(6): 48-56. |
[6] |
WANG Pu,LI Shaoxiang,CHEN Lie,CHEN Xiqing,. Investigation of mold metallurgical behavior under #br# electromagnetic stirring for round bloom[J]. Iron and Steel, 2019, 54(8): 82-89. |
|
|
|
|