Improving internal quality research of the medium carbon steel of[?380 mm]round blooms |
CHENG Fang bo, WANG Guo cai |
(Masteel- Special Steel Company, Maanshan 243000 Anhui, China) |
|
|
Abstract The bloom casting machine have three sections of electromagnetic stirring (M-EMS+S-EMS+F-EMS), Masteel-Special Steel Company. In order to get the best parameter and improved internal quality. Shoot nail experiment near the S-EMS and F-EMS electromagnetic stirring zone. According to the test results of Shoot nail experiment, Simulation calculated the thickness of the shell on the electromagnetic stirring zone. According to the ideal target shell thickness, Simulation process parameters, Design the process optimization experimental program. The 380 mm round billet of medium carbon steel, optimum parameter can be attained and internal quality be improved, based on the contrast analysis about the macro-structure and composition segregation. to reduce the central segregation and shrinkage defects.
|
Received: 13 March 2017
Published: 14 November 2017
|
|
|
|
[1] |
张宏丽,王思刚。搅拌器的结构参数对钢液内电磁场和流场分布的影响[J].钢铁研究学报,2002,14(4):10-15.
|
[2] |
毛斌,陶金明,蒋桃仙。方坯连铸电磁搅拌技术应用中的几个重要问题 [J].炼钢,2008,24(4):16-20.
|
[3] |
巩文旭,贺建哲,刘锦强。82B方坯连铸末端电磁搅拌位置优化研究 [J].天津冶金,2007(4):21.
|
[4] |
李建超,王宝峰,王晓东,等。连铸圆坯凝固末端电磁搅拌位置及工艺参数优化 [J].特种钢铸造及有色合金,2014,34(8):853.
|
[5] |
Oh K S,Chang Y W ,Macro segregation Behavior in Continuously Cast High Carbon Steel Blooms and Billets at the Final Stage of solidification in Combination Stirring [J]. ISU International,1995,35(7):866.
|
|
|
|