Abstract��Second��level pure titanium heat exchanger pipe began to leak after four months operation. By physical and chemical testing and comprehensive analysis, it is suggest that deposited sands and rubber relics lead to local clogging of the pipe, so vortex around the clog lead to erosion abrasion.