Abstract:The residual stress test of multi-manufacturer and multi-specification super13Cr tubing was carried out by using the commonly used blind hole method and ring cutting method,and 36 sets of residual stress test data were obtained. Based on the principle of statistics,the correlation analysis of residual stress obtained by the two methods was carried out.The results showed that there was a strong correl ation between the blind-hole technology and the ring method,and the result of the residual stress by blind-hole technology is about 20% different from the ring method.
熊茂县,杨莎莎,谢俊峰,姬丙寅,马磊,史交齐. 盲孔法与环切法测试油管残余应力相关性探讨[J]. 物理测试, 2019, 37(3): 33-35.
XIONG Mao-xian, YANG Sha-sha, XIE Jun-feng, JI Bing-yin, MA Lei, SHI Jiao-qi. Discussion about correlation between blind-hole technology and the ring method in testing residual-stress of oil casing. PHYSICS EXAMINATION AND TESTING, 2019, 37(3): 33-35.