Causes Analysis of End Cracks and Damaged Top of Steel T8 |
ZHANG Yan-dong,JIANG Tai-qiong,HE Xiao-lin,HE Wen-cheng,HOU Ping-jie,LI Ming-lin |
Xining Special Steel Group Co., Xining 810005, Qinghai, China |
|
|
Abstract When cold shearing was applied on steel T8, there were larger proportion end cracks and damaged top on the steel T8 produced by Plant A. While on the steel of Plant B, the percentage is small. Therefore, the same sized steel T8 were chosen from both Plants and investigation was conducted on their chemical compositions, non-metallic inclusions, brinell hardness and metallographic structure. The results showed that the reason of end cracks by cold cutting is due to its high hardness. High carbon content in the steel resulted in high hardness of steel T8 manufactured by Plant A. Besides, the lower final rolling temperature, longer staying over on cooling beds after rolling and lower pile-cooling temperature all contributed to make the problem worse. However, the internal quality of the steel has no effect on it.
|
Received: 26 March 2013
Published: 17 April 2014
|
|
|
|
[1] |
FENG Hao��JIANG Zhou-hua��LI Hua-bing��HAN Yu��LUO Yi��DING Wei. Influence of austenitizing temperature on microstructure and mechanical properties of high nitrogen bearing steel 30Cr15Mo1N[J]. Chinese Journal of Iron and Steel, 2017, 52(9): 92-98. |
[2] |
GAO Fei-fei����WANG Jing-zhong��BAO Han-sheng. Influence of the laser quenching process parameters on the depth and the hardness of the hardening layer of HT210[J]. Chinese Journal of Iron and Steel, 2017, 35(5): 20-25. |
[3] |
LIU Bao-long����ZHANG Hui-fang��XIAO Zhen-xing��[LU]Zhi-qing��FU Wan-tang��REN Ting-zhi. Microstructure evolution and properties of interface in 316L/Q345R hot rolled clad plate[J]. Chinese Journal of Iron and Steel, 2017, 52(5): 72-76. |
[4] |
HUANG Fei��ZHU Xing-jiang��ZHANG Xiao-li��WU Zhen��WANG Yue. Cause analysis of the fracture of 8Cr5MoV forged steel cold roll[J]. Chinese Journal of Iron and Steel, 2017, 35(4): 42-46. |
[5] |
DAI Xiang-lin������LIU Bao-xi����MA Jiu-le����WEI Jian-yun������YIN Fu-xing����. Microstructure and mechanical properties of stainless steel clad plate fabricated by vacuum hot rolling[J]. Chinese Journal of Iron and Steel, 2017, 52(2): 65-70. |
[6] |
YAN Chun-lian��JIA Hui-ping��JU Xin-hua��QI Qi-ge��WEN Juan. Discussion of determination methods for the decarburization layer depth of 75Cr1 steel[J]. Chinese Journal of Iron and Steel, 2017, 35(2): 35-38. |
|
|
|
|