2022, Vol. 40(3): 31-34 DOI: 10.13228/j.boyuan.issn1001-0777.20210052 | ||
Formation analysis of white spot imperfections on
cold rolling 1Cr18Ni9Ti stainless steel pipes |
||
YU Lei1,YANG Chun1,2,LIU Ming1,2,XIE Jinpeng1,2,ZHONG Zhenqian1,2,ZHANG Zhuo2 | ||
1. NCS Testing Technology Co., Ltd., Beijing 100081, China;
2. Central Iron & Steel Research Institute, Beijing 100081, China |
||
Received 2021-05-06 Revised null | ||
Supporting info | ||
|