RH-KTB optimizing process in production of IF-steel |
Xiao Jiu-lun |
|
|
Abstract The paper briefly introduced the deep-decarbonization principle of RH-KTB based on the practice of product IF-steel in Meishan steel,through ameliorating kinetic conditions to optimize RH-KTB treatment process.By Means of setting 15KPa vacuum degree as the best time to start KTB process,improving vacuum degree of RH and improving circular flow , we could control the RH end-point carbon content of IF steel from 18×10-6 to less than 15×10-6conditions and optimizing RH-KTB treatment process of ultra low carbon steel. The domestic advanced level of controlling carbon content of ultra low carbon steel was reached.
|
Received: 07 December 2009
|
|
|
|
[1] |
YU Hui-xiang, PAN Ming, YANG De-xin. Behavior of inclusions in ultra-low carbon IF steel during deoxidation and alloying process[J]. Iron and Steel, 2020, 55(6): 46-53. |
[2] |
ZHU Tan-hua, ZHOU Qiu-yue, REN Ying, DUAN Hao-jian, ZHANG Li-feng. Inclusion evolution in IF steel during tundish reoxidation[J]. Iron and Steel, 2020, 55(3): 35-39. |
[3] |
YANG Jie1,YAO Hai-ming2,WU Zhen-gang1,GAO Qian-yun2. Clogging control of submerged entry nozzle during IF steelproduction by middle-thin slab process[J]. JOURNAL OF IRON AND STEEL RESEARCH , 2020, 32(1): 20-26. |
[4] |
XIAO Pengcheng,ZHAO Maoguo,ZHU Liguang,HE Shengping. Mathematical simulation and experiment on #br# solidification hook of IF steel[J]. Iron and Steel, 2019, 54(7): 49-55. |
[5] |
LIU Lan-xiao,CHEN Ling-feng,GUAN Jian-dong,WU Nai,ZHOU Na,LIU Juan. Analysis of cross striation on the surface of IFsteel[J]. PHYSICS EXAMINATION AND TESTING, 2019, 37(5): 51-55. |
[6] |
ZHU Rui-qi,SONG Xin-li,ZHENG Ai-qin,CHEN Rong-dong,JIA Juan,FAN Li-xia. Strain hardening and microstructure characteristic of high strength IF bearing phosphorus steel[J]. Iron and Steel, 2018, 53(2): 55-59. |
|
|
|
|