Generation Mechanism of Surface Transverse Cracks in Continuous Annealing and Its Control Technology |
BAI Zhen-hua1,SHEN Yan-zhi2,ZHOU Li2,YU Shun-bing3,SHI Xiao-dong1,SI Hong-xin |
1. College of Mechanical Engineering, State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao 066004, Hebei, China 2. Shougang Research Institute of Technology, Beijing 100043, China 3. Shougang Cold Rolling Co., Ltd., Beijng 101304, China |
|
|
Abstract For the problem of the horizontal stripes defect on the strip surface in the continuous annealing process, fully integrated with equipmental and technological features of the continuous annealing line, and based on such four field trials as the impact test of the rolling speed on the horizontal stripe, the impact test of the speed of strip in furnace on the horizontal stripes, the investigation test of furnace-roller’s surface in annealing furnace and the impact test of the tension in furnace on horizontal stripes, the generation mechanism of horizontal stripes defects of the strip in continuous annealing unit were analyzed in detail, and the comprehensive control measures for horizontal strips was put forward. According to actual situation, the relevant technology was applied to the continuous annealing line, and a detailed technical scheme was worked out. The strip surface quality is improved effectively and larger economic benefits are obtained.
|
Received: 19 July 2010
Published: 28 September 2011
|
|
|
|
[1] |
WANG Pu,LI Shaoxiang,CHEN Lie,CHEN Xiqing,. Investigation of mold metallurgical behavior under #br# electromagnetic stirring for round bloom[J]. Iron and Steel, 2019, 54(8): 82-89. |
[2] |
WANG Wei-wei,LIU Liu,LI Guang-ying. Microstructure and properties of high elongation DP980 cold rolled dual phase steel[J]. JOURNAL OF IRON AND STEEL RESEARCH , 2019, 31(12): 1053-1057. |
[3] |
MA Bingzhi1,QI Chunyu1,LOU Decheng1,ZHANG Yudong2. Surface roughness control technology of galvanized sheet skinpass rolling process[J]. Iron and Steel, 2019, 54(10): 91-95. |
[4] |
REN Wei- chao,LI Yang- long,YANG Zhen,LI Guan- xiong,SUN Jian- xin,ZHENG Xiao- fei. Study on strip running deviation at exit of heat section in continuous annealing furnace for cold rolling[J]. , 2018, 30(9): 723-728. |
[5] |
LIU Shun-ming,LI Yang-long,HOU Da-wei,WANG Dao-jin,ZHENG Xiao-fei. Damage investigation and optimization measures of W-shaped radiant tube in continuous annealing furnace[J]. Iron and Steel, 2018, 53(6): 103-107. |
[6] |
LIU Hua-sai,,WU Nai,LI Zhen,HAN Yun,. Flattening cracking cause and its mechanism analysis of the continuous annealed DP1000 steel[J]. , 2018, 36(6): 35-40. |
|
|
|
|