Analysis on pseudo-eutectoid pearlite in the low carbon steel |
Lü Chang-bao |
Tangshan Branch, Hebei Iron and Steel Co., Ltd., Tangshan 063016, Hebei, China |
|
|
Abstract The metallurgical structure of the specimens with higher strength is detected by optical microscope, and there is more than 50% pseudo-eutectoid pearlite in the specimens, resulting in an effect of remarkable pearlite strengthening. Conclusion of comparative analysis of different process is that far more than balance content of pseudo-eutectoid pearlite can be gotten by inhibiting proeutectoid ferrite transformation and making final cooling temperature lower than the [Ar1] of air cooling. The factors influencing the proeutectoid ferrite transformation during laminar cooling are discussed in this study.
|
Received: 11 July 2014
Published: 18 March 2015
|
|
|
|
[1] |
王有铭,李曼云,韦光.控制轧制与控制冷却[M]. 北京:冶金工业出版社,1995.
|
[1] |
王有铭,李曼云,韦光.控制轧制与控制冷却[M]. 北京:冶金工业出版社,1995.
|
[2] |
崔忠圻,覃耀春.金属学与热处理[M]. 北京:机械工业出版社,2007.
|
[2] |
崔忠圻,覃耀春.金属学与热处理[M]. 北京:机械工业出版社,2007.
|
[3] |
威廉.劳斯特克,詹姆斯R.德弗莱克. 金相组织解说[M]. 上海:上海科学技术出版社,1984.
|
[3] |
威廉.劳斯特克,詹姆斯R.德弗莱克. 金相组织解说[M]. 上海:上海科学技术出版社,1984.
|
[4] |
朱祖昌,许雯.钢中珠光体转变一[J].热处理技术与装备, 2011, 32(3):65-70
|
[4] |
朱祖昌,许雯.钢中珠光体转变一[J].热处理技术与装备, 2011, 32(3):65-70
|
[5] |
李文卿,崔文暄.轧后快冷对低碳钢板组织和力学性能的影响[J].钢铁, 1986, 21(2):29-33
|
[5] |
李文卿,崔文暄.轧后快冷对低碳钢板组织和力学性能的影响[J].钢铁, 1986, 21(2):29-33
|
[6] |
李文卿.控冷低碳钢珠光体形貌与退化机制[J].钢铁, 1991, 26(10):30-34
|
[6] |
李文卿.控冷低碳钢珠光体形貌与退化机制[J].钢铁, 1991, 26(10):30-34
|
[7] |
王连伟,毛征东.过冷奥氏体转变温度对钢珠光体退化的影响[J].钢铁, 2002, 37(2):47-51
|
[7] |
王连伟,毛征东.过冷奥氏体转变温度对钢珠光体退化的影响[J].钢铁, 2002, 37(2):47-51
|
[8] |
王立军,蔡庆伍,余伟,等.低碳低合金钢的连续冷却相变组织特征及其形成机制[J].材料工程, 2010, (8):29-33
|
[8] |
王立军,蔡庆伍,余伟,等.低碳低合金钢的连续冷却相变组织特征及其形成机制[J].材料工程, 2010, (8):29-33
|
[1] |
YAN Xue-qiang1,2,ZHENG Wan1,2,WANG Guo-wei1,2,YAN Wen1,LI Guang-qiang1,2. Effect of microporous MgO refractories on steel cleanliness[J]. JOURNAL OF IRON AND STEEL RESEARCH , 2020, 32(6): 483-490. |
[2] |
YUAN Peng,,ZHANG Jun,LIU Dao-zheng,LI Hai-bo,,ZHU Ke-ran,CHEN Bin,. Formation mechanism and control technology of Al-Ti inclusions in ultra low carbon steel[J]. Iron and Steel, 2018, 53(7): 24-30. |
[3] |
WEN Guo-dong,LIU He-jia. Analysis and solution for the cracking of ERW welded pipe[J]. , 2018, 36(5): 36-39. |
[4] |
LU Heng-chang,HU Chun-dong,WANG Cun-yu,PU En-xiang,LIU Jian-hui,DONG Han,. Kinetics of massive transformation for an ultra-low carbon steel containing niobium[J]. Iron and Steel, 2018, 53(2): 50-54. |
[5] |
LI Jiang-hua,ZHAO Zheng-yu,YANG Hui,YANG Pei-hong,LI Man-lin. Tensile strain aging behavior of low carbon steel with different nitrogen content[J]. , 2018, 36(1): 12-15. |
[6] |
WANG Li,,LI Guang- qiang,,,LIU Yu,,ZHANG Zhao,,LI Ya- wei,XU Xiao- feng. Interaction between ultra- low carbon liquid steel and MgO- C refractories containing different carbon contents[J]. Chinese Journal of Iron and Steel, 2017, 29(8): 616-625. |
|
|
|
|