Abstract:After analyzing the surface cracks of 1Cr11MoV stainless steel continuous cast slab produced by TISCO 1 280 mm continuous casting, measures like controlling molten steel superheat, altering mold cooling strength, secondary cooling water, carbon content and fluxes were put forward so that the horizontal cracks were reduced significantly.
收稿日期: 2011-09-05
出版日期: 2012-03-26
引用本文:
范新智. 1Cr11MoV板坯表面纵裂原因分析及改进措施[J]. 中国钢铁期刊网, 2012, 31(2): 45-47.
FAN Xin-zhi. Cause Analysis and Countermeasures of 1Cr11MoV Stainless Steel Continuous Cast Slab Surface Cracks. Chinese Journal of Iron and Steel, 2012, 31(2): 45-47.