Abstract:For the problems of surface indentation defect and ovality defect occurred from larger mechanical deformation in round bloom casting, with the comprehensive consideration of the balance design between withdrawal resistance and downslide force, the rule for establishment of hot strand pressure had been developed. It was shown that the reliability on control ovality defect from larger surface indentation had been verified.
韩占光. 圆坯连铸热坯压力设计方法及实践[J]. 中国钢铁期刊网, 2015, 34(1): 53-56.
HAN Zhan-guang. Design and practice of hot-strand pressure for round bloom continuous casting. Chinese Journal of Iron and Steel, 2015, 34(1): 53-56.