Abstract:For non-oriented silicon steel 50W800 with RH process, there were plentiful inclusions, researchers employed SEM-EDS method to analyze the size, quantity and type of inclusions, and detected the constituents of slag. Results showed that Ar blowing could get rid of 39.11% inclusions, and the total area of inclusions reduced 2 406.94 μm2 from RH to tundish. The majority of inclusions were Al2O3 sized between 1-4 μm, and there existed a small amount of AlN?Al2O3 and CaO-Al2O3-MgO compound inclusions. Slag owned an excellent capability to absorb the inclusions, but the modification effect was not evident.
赤小浩,李康伟. 无取向硅钢精炼过程夹杂物控制研究[J]. 中国钢铁期刊网, 2016, 35(1): 14-17.
CHI Xiao-hao,LI Kang-wei. Research of inclusions in RH refined process of non-oriented silicon steel 50W800. Chinese Journal of Iron and Steel, 2016, 35(1): 14-17.