Abstract:Through the analysis of cleanliness, unsteady casting of DC06 steel in the production process the results show that the head slab 2.5 m after inclusion content of casting billet tends to be stable, close to the 3.0 mg/10 kg normal level is higher than the level of normal slab billet; large inclusion content transfer blank, mainly containing Ti and Zr of the Al2O3-CaO class with content level; the fluctuation of the large inclusions in the slab, close to the normal level of billet; nozzle change when the large inclusions in the slab billet was significantly higher than the normal level, reached more than 20mg/kg, the inclusions are mainly spherical alumina inclusion, source water mouth clogging.
收稿日期: 2017-03-30
出版日期: 2017-09-27
引用本文:
张春杰. 非稳态浇铸对DC06钢种洁净度的影响分析[J]. 中国钢铁期刊网, 2017, 36(04): 21-25.
ZHANG Chun-jie. Analysis of the influence of DC06 steel cleanliness unsteady casting. Chinese Journal of Iron and Steel, 2017, 36(04): 21-25.