Analysis of corrosion resistance of 445J2 ferrite stainless steel |
REN Juanhong1, CHEN Anzhong1, GAO Renqiang1, PAN Jixiang2 |
1. Research Institute, JISCO, Jiayuguan 735100, China; 2. Stainless Steel Branch, JISCO, Jiayuguan 735100, China |
|
|
Abstract The microstructure and corrosion resistance of ultra-pure ferritic stainless steel 445J2 and austenitic stainless steel 316L were studied by means of microstructure analysis, tensile test, salt spray corrosion test, electrochemical test, and stress corrosion test. The results showed that 445J2 stainless steel had low work hardening orientation and good deep drawing formability. Compared with 316L, the 445J2 stainless steel had lower density, better thermal conductivity, smaller coefficient of thermal expansion, less thermal deformation, better salt spray corrosion resistance and pitting corrosion resistance. Moreover, it had no intergranular corrosion sensitivity and stress corrosion tendency. The 445J2 stainless steel could replace 316L austenitic stainless steel for the application in water system, building roof, curtain wall and many other fields with high corrosion resistance requirements.
|
Received: 02 June 2022
|
|
|
|
[1] |
游香米,姜周华,李花兵,等.超纯铁素体不锈钢的开发与应用现状[J]. 中国冶金,2006,16(11):16.
|
[2] |
陆世英. 不锈钢概论[M]. 北京:化学工业出版社,2013.
|
[3] |
杨献金,姜志祥. 445铁素体不锈钢内胆水箱的加工性能和耐蚀性[J]. 腐蚀与防护,2012,33(7):630.
|
[4] |
毕洪运. 晶界工程抑制SUS304不锈钢晶界贫铬机制[J]. 钢铁,2005,40(6):68.
|
[5] |
于耀,白琴,夏爽,等. 晶界工程处理对316和316L奥氏体不锈钢耐晶间腐蚀性能的影响[J]. 上海金属,2021,43(3):13.
|
[6] |
高中平,陈范才,赵常就. EPR法评价晶间腐蚀敏感性的各种判据的比较[J]. 中国腐蚀与防护学报,2000,20(4):243.
|
[7] |
张晓丹,刘志文,徐海峰,等. 电解抛光质量对高氮不锈钢析出相原子力显微镜形貌表征的影响[J].物理测试,2022,40(6):11.
|
[8] |
卫海瑞,杨永超. 某洗衣机内筒用430不锈钢锈蚀原因分析[J].物理测试,2022,40(1):51.
|
[1] |
SHANG Shuohua, ZOU Chong, LI Jianyun, SHE Yuan, LIU Shiwei, SHI Ruimeng. Intervention degree of tamping process on properties of coke based on petrographic analysis of coal[J]. Iron and Steel, 2023, 58(6): 26-35. |
[2] |
HONG Lukuo, AI Liqun, SUN Caijiao, MENG Fanjun, WANG Xufeng, TONG Shuai. Microstructure evolution and mechanical properties of manganese steel during solid state decarburization[J]. Iron and Steel, 2023, 58(6): 118-125. |
[3] |
WAN Zhi-jian, ZHAO Hai, LIU Xue-hua, ZHANG Jian. Effect of V on microstructure and mechanical properties of wheel steel[J]. Iron and Steel, 2023, 58(5): 104-111. |
[4] |
HONG Lu-kuo, AI Li-qun, SUN Cai-jiao, LI Ya-qiang, ZHOU Mei-jie, MENG Fan-jun. Preparation of medium manganese steel high strength plastic with composition gradient by solid state decarbonization[J]. Iron and Steel, 2023, 58(5): 131-136. |
[5] |
YANG Yong-kun, ZHU Jia-yu, LI Xiao-ming, WANG Yang, ZHAN Dong-ping. A review of research on banded structure control in low carbon alloy steel[J]. Iron and Steel, 2023, 58(4): 1-10. |
[6] |
CHEN Mi-da, ZHANG Yun-xiang, LIANG Feng-rui, ZHOU Nai-peng, CHEN Shi. Effect of C and N contents on mechanical properties of tempered large size bulb flat steel[J]. Iron and Steel, 2023, 58(4): 126-137. |
|
|
|
|