Cause analysis and improvement of brittle fracture #br# of HRB400 hot rolled ribbed steel bar | ||
XU Yan,GUO Zhan,WANG Debao,SONG Zufeng | ||
Maanshan Iron and Steel Co., Ltd.,Ma′anshan 243001, China | ||