Abstract:In order to evaluate the effects of Si on oxidation kinetics behavior of steels, the oxidation behaviors of Fe-0.2Si steel and Fe-2Si steel at 900-1 200 ℃ in the air-steam atmosphere were investigated by TGA in order to calculate the oxidation rates of two steels. The activation energies of the two steels were obtained. The results show that the oxidation kinetics cures of the two steels obey linear law in the early stage of oxidation process. It appeared that a critical thickness of scale existed,at which the law of the scale-growth mechanism changed from linear to parabolic. The critical thickness of scale increased with the silicon mass percent in the steel increasing and the temperature rising.
收稿日期: 2018-03-06
出版日期: 2018-10-11
引用本文:
孙 彬,尤宏广,郝明欣. 0.09C-0.5Mn-0.22/1.9Si钢的高温氧化动力学[J]. , 2018, 53(9): 53-56.
SUN Bin,YOU Hong-guang,HAO Ming-xin. Kinetics of high temperature oxidation of 0.09C-0.5Mn-0.22/1.9Si steel. Iron and Steel, 2018, 53(9): 53-56.
Zhu Z, Xu H, Jiang D, et al. Influence of temperature on the oxidation behaviour of a ferritic-martensitic steel in supercritical water[J]. Corrosion Science, 2016, 113:172-179
[1]
Zhu Z, Xu H, Jiang D, et al. Influence of temperature on the oxidation behaviour of a ferritic-martensitic steel in supercritical water[J]. Corrosion Science, 2016, 113:172-179
[2]
Rex Y. Chen,W. Y. D. Yuen. Short-time Oxidation Behavior of Low-carbon, Low-silicon Steel in Air at 850–1,180℃––I:Oxidation Kinetics[J]. Oxidation of Metals,2008,70(1):39-68.
[2]
Rex Y. Chen,W. Y. D. Yuen. Short-time Oxidation Behavior of Low-carbon, Low-silicon Steel in Air at 850–1,180℃––I:Oxidation Kinetics[J]. Oxidation of Metals,2008,70(1):39-68.
[3]
Pieraggi B, Rolland C, Bruckel P. Morphological characteristics of oxide scales grown on H11 steel oxidised in dry or wet air[J]. Materials at High Temperatures, 2005, 22(22):61-68.
[3]
Pieraggi B, Rolland C, Bruckel P. Morphological characteristics of oxide scales grown on H11 steel oxidised in dry or wet air[J]. Materials at High Temperatures, 2005, 22(22):61-68.
[4]
KofstadP.Prediction the Numerical Model of Metal Non Isothermal Oxidation Kinetics[J].Acta Chemical Scandinavica,1958,12(2):701.
[4]
KofstadP.Prediction the Numerical Model of Metal Non Isothermal Oxidation Kinetics[J].Acta Chemical Scandinavica,1958,12(2):701.
[5]
S.NevioBalo,F.Yakuphanoglu. The effects of Cr on isothermal oxidation behavior of Fe-30Mn-6Si alloy[J].Thermochimica Acta,2013(560):43-46.
[5]
S.NevioBalo,F.Yakuphanoglu. The effects of Cr on isothermal oxidation behavior of Fe-30Mn-6Si alloy[J].Thermochimica Acta,2013(560):43-46.
[6]
刘小江,李振宇.热轧无取向硅钢高温氧化行为及其氧化铁皮控制技术的研究与应用 [D]. 沈阳:东北大学,2014Liu Xiaojiang, Li Zhenyu. Reseach on High Tempreture Oxidation Behavior and Countrolling Technology and Application of Oxide Scale of Hot-rolled Non-oriented Silicon Steel[D]. Shenyang: Northeastern University,2014.
[6]
刘小江,李振宇.热轧无取向硅钢高温氧化行为及其氧化铁皮控制技术的研究与应用 [D]. 沈阳:东北大学,2014Liu Xiaojiang, Li Zhenyu. Reseach on High Tempreture Oxidation Behavior and Countrolling Technology and Application of Oxide Scale of Hot-rolled Non-oriented Silicon Steel[D]. Shenyang: Northeastern University,2014.
[7]
Rex Y. Chen,W. Y. D. Yuen. Short-Time Oxidation Behavior of Low-Carbon,Low-Silicon Steel in Air at 850–1180 _C: II. Linear to Parabolic Transition Determined Using Existing Gas-Phase Transport and Solid-Phase Diffusion Theories[J].Oxidation of Metals, 2010, 73(1): 353 -373.
[7]
Rex Y. Chen,W. Y. D. Yuen. Short-Time Oxidation Behavior of Low-Carbon,Low-Silicon Steel in Air at 850–1180 _C: II. Linear to Parabolic Transition Determined Using Existing Gas-Phase Transport and Solid-Phase Diffusion Theories[J].Oxidation of Metals, 2010, 73(1): 353 -373.
[8]
W.Y.D.Yuen, R.Y.Chen. Short-time Oxidation Behavior of Low-carbon, Low-silicon Steel in Air at 850–1,180 _C—III: Mixed Linear-and-Parabolic to Parabolic Transition Determined Using Local Mass-Transport Theories[J].Oxidation of Metals, 2010, 74(1):255-274.