Development of comprehensive optimum setting technology for roll profile curve of continuous annealing unit
BAI Zhen-hua1,2, XU Peng1, WANG Xiao-lei1, HE Zhao-long1, WANG Yun-xiang1
1. National Engineering Research Center for Equipment and Technology of CSR, Yanshan University, Qinhuangdao 066004, Hebei, China 2. State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao 066004, Hebei, China
Abstract:Aiming at the problem that the design process of roll profile curve optimization of continuous annealing units in the past only considers the stability of the through plate, not the shape control,and only adopts the separate optimization of process sections without considering the coordinated setting of the whole furnace section. On the basis of a large number of field tests and theoretical studies,considering not only the stability of the through plate of the continuous annealing unit but also the shape control,but also the organic relationship between the upstream and downstream process sections in the furnace,the corresponding objective function of roll profile optimization is constructed,and a set of comprehensive optimum setting technology for roll profile curve of whole furnace section suitable for continuous annealing unit is put forward,which is applied to the production practice of a 1 550 continuous annealing unit and achieved good results. It has effectively improved the stability of the through plate and the quality of the exit plate of the unit. It has created greater economic benefits for the site and has the value of further popularization and application.
白振华, 许鹏, 王晓雷, 何召龙, 王云祥. 连退机组炉辊辊型曲线综合优化设定技术开发[J]. 钢铁, 2019, 54(12): 48-54.
BAI Zhen-hua, XU Peng, WANG Xiao-lei, HE Zhao-long, WANG Yun-xiang. Development of comprehensive optimum setting technology for roll profile curve of continuous annealing unit. Iron and Steel, 2019, 54(12): 48-54.
黄海生. 新钢连退炉内张力控制优化[J]. 轧钢,2016,33(5):84.(HUANG Hai-sheng.Tension control optimization in continuous withdrawal of Xingang[J]. Steel Rolling,2016,33(5):84.)
[2]
卢秉仲,张霞,王亚东.薄规格超宽幅汽车板连退热瓢曲控制和优化[J].轧钢,2018,35(3):37.(LU Bing-zhong,ZHANG Xia,WANG Ya-dong.Control and optimization of continuous cooling ladle bending of thin gauge ultra-wide automobile plate[J].Steel Rolling,2018,35(3):37.)
[3]
王少飞,唐伟,窦爱民,等.提高CVC冷连轧机板形控制能力的新工艺技术[J].冶金自动化,2018,42(3):42.(WANG Shao-fei, TANG Wei, DOU Ai-min,et al.New process technology for improving strip shape control ability of CVC cold tandem rolling mill[J].Metallurgical Automation, 2018,42(3):42.)
[4]
张君,张岩岩,兴百宪,等.基于辊径方差最小的三次CVC辊型参数设计方法[J].轧钢,2017,34(5):41.(ZHANG Jun, ZHANG Yan-yan, XING Bai-xian,et al.Design method of cubic CVC roll profile parameters based on minimum variance of roll diameter[J].Steel Rolling,2017,34(5):41.)
[5]
白振华,陈双玉,钱承,等.连续退火过程带钢跑偏模型及其影响因素[J].塑性工程学报,2016,23(2):28.(BAI Zhen-hua,CHEN Shuang-yu,QIAN Cheng,et al.Strip deviation model during continuous annealing process and its influencing factors[J].Journal of Plastic Engineering,2016,23(2):28.)
[6]
王瑞. 连续退火过程带钢稳定通板综合控制技术研究[D].秦皇岛:燕山大学,2017.(WANG Rui.Research on Integrated Control Technology of Strip Stable Pass Plate in Continuous Annealing Process[D].Qinhuangdao:Yanshan University,2017.)
[7]
靳振伟,滕洪宝,张长利,等.高强钢SFB700热轧板形缺陷的成因及控制措施[J].中国冶金,2018,28(7):50.(JIN Zhen-wei,TENG Hong-bao,ZHANG Chang-li,et al.Causes and control measures of shape defects in SFB700 hot rolled high strength steel[J].China Metallurgy,2018,28(7):50.)
[8]
邵健,何安瑞,孙文权,等.面向生产全过程的热轧带钢精准控制核心技术[J].中国冶金,2017,27(5):45.(SHAO Jian,HE An-rui,SUN Wen-quan,et al.Core technology of precise control for hot rolled strip for the whole production process[J].China Metallurgy,2017,27(5):45.)
[9]
刘华强,杨荃,王晓晨,等.热轧宽带钢工作辊磨损辊型预报模型及应用[J].轧钢,2018,35(4):45.(LIU Hua-qiang,YANG Quan,WANG Xiao-chen,et al.Prediction model and application of work roll wear profile of hot rolled broadband steel[J].Steel Rolling,2018,35(4):45.)
[10]
郑海燕,王道金,刘顺明,等.冷轧连退炉内带钢跑偏控制[J].轧钢,2017,34(5):86.(ZHENG Hai-yan,WANG Dao-jin,LIU Shun-ming,et al.Strip deviation control in cold rolling continuous stripping furnace[J].Steel Rolling,2017,34(5):86.)
[11]
刘顺明,李冠雄,任秋红,等.宽幅带钢初始板形及跑偏机理研究[J].轧钢,2018,35(3):49.(LIU Shun-ming,LI Guan-xiong,REN Qiu-hong,et al.Initial shape and deviation mechanism of wide strip[J].Steel Rolling,2018,35(3):49.)
[12]
杨静,唐荻,苏岚,等.双锥度辊辊形参数对带钢瓢曲变形的影响[J].北京科技大学学报,2010,32(9):1215.(YANG Jing,TANG Di,SU Lan,et al.Effect of roll shape parameters of double taper rolls on bending deformation of strip steel[J].Journal of Beijing University of Science and Technology,2010,32(9):1215.)
[13]
杨静,杨进,李卫杰.连退炉内炉辊的选择与优化设计[J].工业炉,2011,33(6):23.(YANG Jing,YANG Jin,LI Wei-jie.Selection and optimum design of rollers in continuous removal furnace[J].Industrial Furnace,2011,33(6):23.)
[14]
李志伟. 连续退火机组炉辊辊型的设计与选择[J].鞍钢技术,2007(13):33.(LI Zhi-wei.Design and selection of roll profile for continuous annealing unit[J].Angang Technology,2007(13):33.)
[15]
杨士弘,杨海水,张鹏,等.连续退火炉中带钢跑偏分析[J].河北冶金,2017(12):47.(YANG Shi-hong,YANG Hai-shui,ZHANG Peng,et al.Analysis of strip deviation in continuous annealing furnace[J].Hebei Metallurgy,2017(12):47.)
[16]
白振华,王云祥,王瑞,等.连续退火机组炉内炉辊辊型综合优化技术[J].中国机械工程,2017,28(14):1759.(BAI Zhen-hua,WANG Yun-xiang,WANG Rui,et al.Comprehensive optimization technology of roll profile in furnace of continuous annealing unit[J].China Mechanical Engineering,2017,28(14):1759.)
[17]
白振华,王云祥,王瑞,等.连退过程炉辊粗糙度衰减模型及张应力补偿技术[J].塑性工程学报,2017,24(6):129.(BAI Zhen-hua,WANG Yun-xiang,WANG Rui,et al.Roughness attenuation model and tensile stress compensation technology of rollers in continuous retreat process[J].Journal of Plastic Engineering,2017,24(6):129.)
[18]
李维特,黄保海.热应力理论分析及应用[M].北京:中国电力出版社,2004.(LI Wei-te,HUANG Bao-hai.Thermal Stress Theory Analysis and Application[M].Beijing:China Electric Power Press,2004.)
[19]
李明,陈世恒.连续退火炉区带钢跑偏原因分析与控制[J].轧钢,2018,35(5):88.(LI Ming,CHEN Shi-heng.Cause analysis and control of strip deviation in continuous annealing furnace area[J].Steel Rolling,2018,35(5):88.)
[20]
白振华,王瑞,张岩岩,等.连退过程中带钢板形在线控制技术[J].钢铁,2016,51(2):62.(BAI Zhen-hua,WANG Rui,ZHANG Yan-yan,et al.On-line control technology of strip shape during continuous retreat[J].Iron and Steel,2016,51(2):62.)
[21]
王瑞,白振华,王云祥, 等.连退过程带钢热瓢曲指数及其影响因素[J].钢铁,2016,51(12):94.(WANG Rui,BAI Zhen-hua,WANG Yun-xiang,et al.Hot ladle bending index of strip steel and its influencing factors during continuous retreat[J].Iron and Steel,2016,51(12):94.)
[22]
王鹏涛. Powell寻优法及其应用[J].系统工程理论与实践,1997(9):64.(WANG Peng-tao.Powell optimization method and its application[J].System Engineering Theory and Practice,1997(9):64.)