Research status and prospect of fatigue life of hollow drill steel
HAN Yi1, ZHANG Long1, XIAO Yao1, YU En-lin1, WANG Qing-liang1, ZHAO Yu-qian2
1. National Engineering Research Center for Equipment and Technology of Cold Rolling Strip, Yanshan University, Qinhuangdao 066004, Hebei, China; 2. School of Control Engineering,Northeastern University at Qinhuangdao, Qinhuangdao 066004, Hebei, China
Abstract:Hollow drill steel is a special steel material for manufacturing rock drill rod and also a representative product of rock drill steel industry. All the hollow drill steel used in the high quality rock drill tools around the world has high fatigue life and stable quality,which is fine steel with high technology and high value-added. Compared with imported high-end hollow drill steel,the fatigue life of domestic hollow steel of the same type still has a large room for improvement. China is a major producer and user in the rock drill steel and tools industry,in order to achieve high-quality development,the new technology and process of steel industry will be used for reference,and the new method to improve the fatigue life of hollow drill steel will be explored to produce high-quality hollow drill steel with high fatigue life and stable quality. In view of the failure form of hollow drill steel and the main factors that affect its fatigue life,the present research results of improving and estimating its fatigue life are reviewed. In the future,the advanced technology such as electromagnetic stirring,electropulsing treatment will be used to further improve the quality of hollow drill steel,the application conditions of the combination of the intelligent prediction and management system of fatigue life and the technology of crack repairing will be developed.
韩毅, 张龙, 肖瑶, 于恩林, 王青亮, 赵玉倩. 中空钢疲劳寿命的研究现状及展望[J]. 钢铁, 2020, 55(9): 1-10.
HAN Yi, ZHANG Long, XIAO Yao, YU En-lin, WANG Qing-liang, ZHAO Yu-qian. Research status and prospect of fatigue life of hollow drill steel[J]. Iron and Steel, 2020, 55(9): 1-10.
[1] 王国栋,吴迪,朱苗勇,等. 后工业化时代的生态化轧钢工艺技术:钢铁共性技术协同创新中心工艺与装备开发平台简介[J]. 中国冶金,2014,24(11):1.(WANG Guo-dong,WU Di,ZHU Miao-yong,et al. Ecological rolling technology in the postindustrial era:Platform of process and equipment of steel generic technology and innovation center[J]. China Metallurgy,2014,24(11):1.) [2] 李新创. 新时代钢铁工业高质量发展之路[J]. 钢铁,2019,54(1):1.(LI Xin-chuang. Road map to high-quality development of iron and steel industry in new age[J]. Iron and Steel,2019,54(1):1.) [3] 洪达灵,顾太和,徐曙光,等. 钎钢与钎具[M]. 北京:冶金工业出版社,2000.(HONG Da-ling,GU Tai-he,XU Shu-guang,et al. Drill Steel and Drill Tool[M]. Beijing:Metallurgical Industry Press,2000.) [4] 张国榉. 高铁网、地球村、大同梦[J]. 凿岩机械气动工具,2016(4):1.(ZHANG Guo-ju. HSR network,global village and dream of great harmony[J]. Rock Drilling Machines and Pneumatic Tools,2016(4):1.) [5] 胡铭,董鑫业. 我国钎钢钎具产业现状及对发展的建议[J]. 凿岩机械气动工具,2015(1):7.(HU Ming,DONG Xin-ye. Advice on development and status of rock drill steels and tools in China[J]. Rock Drilling Machines and Pneumatic Tools,2015(1):7.) [6] 于恩林,韩毅,肖瑶. 钎钢成形与冷却数值计算[M]. 沈阳:东北大学出版社,2019.(YU En-lin,HAN Yi,XIAO Yao,et al. Numerical Calculation of Forming and Cooling of Rock Drill Steel[M]. Shenyang:Northeast University Press,2019.) [7] 黄宇,谢有,成国光. 国内外23CrNi3Mo钎具钢洁净度的差异[J]. 中国冶金,2018,28(8):10.(HUANG Yu,XIE You,CHENG Guo-guang. Comparing cleanliness of 23CrNi3Mo hollow drill steel at home and abroad[J]. China Metallurgy,2018,28(8):10.) [8] 王林珠,李京社,熊家泽,等. 国内外95CrMo中空钢成品洁净度及组织性能分析[J]. 中国冶金,2014,24(12):5.(WANG Lin-zhu,LI Jing-she,XIONG Jia-ze,et al. Analysis on cleanness,microstructure and properties of the finished hollow steel 95CrMo product from domestic and abroad[J]. China Metallurgy,2014,24(12):5.) [9] 张波,李高盛,熊家泽,等. 改善95CrMo钢强塑性的热变形工艺[J]. 金属热处理,2016,41(2):136.(ZHANG Bo,LI Gao-sheng,XIONG Jia-ze,et al. Hot forming process for improving strength and ductility of 95CrMo steel[J]. Heat Treatment of Metals,2016,41(2):136.) [10] 闫永明,刘雅政,周乐育,等. 热处理工艺对23CrNi3Mo钎具钢组织及性能的影响[J]. 材料热处理学报,2014,35(2):110.(YAN Yong-ming,LIU Ya-zheng,ZHOU Le-yu,et al. Influence of heat treatment process on microstructure and properties of 23CrNi3Mo steel[J]. Transactions of Materials and Heat Treatment,2014,35(2):110.) [11] 于恩林,赵玉倩,刘辉,等. 钎钢轧制过程主要工艺参数对成品质量的影响[J]. 中国机械工程,2007(18):2249.(YU En-lin,ZHAO Yu-qian,LIU Hui,et al. Influences of processing parameters on final product quality in rock drill steel rolling [J]. China Mechanical Engineering,2007(18):2249.) [12] 黎炳雄,洪达灵. 钎钢内壁强化的初步研究[J]. 现代机械,1979(2):38.(LI Bing-xiong,HONG Da-ling. Study on strengthening of inner wall of rock drill steel[J]. Modern Machinery,1979(2):38.) [13] 闫永明,刘雅政,周乐育,等. 钎具钢23CrNi3Mo渗碳规律及显微组织研究[J]. 材料科学与工艺,2013,21(5):102.(YAN Yong-ming,LIU Ya-zheng,ZHOU Le-yu,et al. Carburizing law and microstructure of 23CrNi3Mo drill steel[J]. Materials Science and Technology,2013,21(5):102.) [14] 秦少杰,梁益龙,邹雄. 磨料水喷丸对23CrNi3Mo钢高周疲劳性能的影响[J]. 金属热处理,2019,44(5):110.(QIN Shao-jie,LIANG Yi-long,ZOU Xiong. Effect of high-energy abrasive waterjet peening on high-cycle fatigue behavior of 23CrNi3Mo steel[J]. Heat Treatment of Metals,2019,44(5):110.) [15] 宋守志,徐小荷,李润隆. 用计算机预估钎杆疲劳寿命的研究[J]. 钢铁,1986,21(3):30.(SONG Shou-zhi,XU Xiao-he,LI Run-long. Study on estimating fatigue life of drill rod by computer[J]. Iron and Steel,1986,21(3):30.) [16] 赵统武,陈仁福,李泽沛,等. 钎钢寿命试验台的研究[J]. 钢铁,1987,22(8):30.(ZHAO Tong-wu,CHEN Ren-fu,LI Ze-pei,et al. A test system for the life of drill steel[J]. Iron and Steel,1987,22(8):30.) [17] Chaijaruwanich A,Thongthip C. Failure analysis of hydraulic rotary drill rods in a limestone mine[J]. International Journal of Mechanical Engineering and Robotics Research,2016,5(4):251. [18] 蔡钢,雷旻,梁益龙,等. B22钎杆断裂失效分析[J]. 矿山机械,2014,42(12):110.(CAI Gang,LEI Min,LIANG Yi-long,et al. Fracture failure analysis of B22 drilling rod[J]. Mining and Processing Equipment,2014,42(12):110.) [19] Mussa A,Krakhmalev P,Bergström J. Failure analyses and wear mechanisms of rock drill rods,a case study[J]. Engineering Failure Analysis,2019,102:69. [20] 顾太和. 冶轧质量对钎钢性能与凿岩寿命的影响[J]. 钢铁,1989,24(8):54.(GU Tai-he. Influence of metallurgical quality of drill steel on its properties and service life[J]. Iron and Steel,1989,24(8):54.) [21] 张国榉,叶凌云,邹文,等. Q22、Q25 mm Cr-Ni-Mo、Cr-Ni-W系列正七边形中空钎钢的研发[J]. 凿岩机械气动工具,2017(3):57.(ZHANG Guo-ju,YE Ling-yun,ZOU Wen,et al. Development of Cr-Ni-Mo,Cr-Ni-W families of Q22 and Q25mm heptagon hollow drilling steels[J]. Rock Drilling Machines and Pneumatic Tools,2017(3):57.) [22] 黄宇,成国光,谢有. 稀土Ce对钎具钢中夹杂物的改质机理研究[J]. 金属学报,2018,54(9):1253.(HUANG Yu,CHENG Guo-guang,XIE You. Modification mechanism of cerium on the inclusions in drill steel[J]. Acta Metallurgica Sinica,2018,54(9):1253.) [23] LI Xiang,WANG Lin-zhu,YANG Shu-feng,et al. Effect of slag composition on the cleanliness of drill rod steel[J]. Ironmaking and Steelmaking,2019,46(5):416. [24] 朱荣,吴学涛,魏光升,等. 电弧炉炼钢绿色及智能化技术进展[J]. 钢铁,2019,54(8):9.(ZHU Rong,WU Xue-tao,WEI Guang-sheng,et al. Development of green and intelligent technologies in electric arc furnace steelmaking processes[J]. Iron and Steel,2019,54(8):9.) [25] ZHANG L,HOU Y,LI Y,et al. Size and type of inclusions in Fe-Cr-Co heat-resistant steel and elevated-temperature strength under the effect of electromagnetic stirring[J]. ISIJ International,2019,59(6):1049. [26] 王筑生,余伟,熊家泽,等. 95CrMo钎具用钢的动态与静态相变研究[J]. 凿岩机械气动工具,2015(2):25.(WANG Zhu-sheng,YU Wei,XIONG Jia-ze,et al. Researches on dynamic and static transformations of 95CrMo drill steel[J]. Rock Drilling Machines and Pneumatic Tools,2015(2):25.) [27] 徐士新,余伟,李舒笳,等. 控轧控冷工艺对钎杆用22Cr-Ni3Mo钢耐磨性能的影响[J]. 热加工工艺,2017,46(19):36. (XU Shi-xin,YU Wei,LI Shu-jia,et al. Effect of controlled rolling and cooling process on wear resistance of 22CrNi3Mo steel for drill rod[J]. Hot Working Technology,2017,46(19):36.) [28] 代利,杨晓,雷旻. 23CrNi3Mo钢的连续冷却转变曲线[J]. 金属热处理,2017,42(3):15.(DAI Li,YANG Xiao,LEI Min. Continuous cooling transformation curves of 23CrNi3-Mo steel[J]. Heat Treatment of Metals,2017,42(3):15.) [29] Zhao M C,Unenbayar T,Zhao Y C,et al. Influence of tempering temperature on the microstructure and mechanical properties of a Cr-Ni-Mo-alloyed steel for rock drill applications[J]. Steel Research International,2019,54:1900297. [30] 余伟,徐士新,王班,等. 22CrNi3Mo超高强钢的直接热处理工艺试验[J]. 材料热处理学报,2015,36(7):48.(YU Wei,XU Shi-xin,WANG Ban,et al. Direct heat treatment process experiment of 22CrNi3Mo ultra high strength steel[J]. Transactions of Materials and Heat Treatment,2015,36(7):48.) [31] 秦晓峰,朱洪武,周乐育,等. FF710钎具钢下贝氏体/马氏体复相组织的控制[J]. 材料热处理学报,2013,34(s2):111.(QIN Xiao-feng,ZHU Hong-wu,ZHOU Le-yu,et al. Control of lower bainite/martensite duplex structure of the FF710 drill steel[J]. Transactions of Materials and Heat Treatment,2013,34(s2):111.) [32] 闫涛. 55SiMnMo中空钢孔型轧制及冷却过程数值模拟与试验研究[D]. 秦皇岛:燕山大学,2014.(YAN Tao. Numerical Simulation and Experimental Study on Grooving Rolling and Cooling Process of 55SiMnMo Hollow Drill Steel[D]. Qinhuangdao:Yanshan University,2014.) [33] 赵玉倩. 钎钢热穿热轧成形过程热力组织模拟及试验研究[D]. 秦皇岛:燕山大学,2012.(ZHAO Yu-qian. Numerical Simulation and Experimental Study on Hot Perforating and Hot Rolling Process of Drilling Steels[D]. Qinhuangdao:Yanshan University,2012.) [34] YU En-lin,YAN Tao,SHEN Hong-wei,et al. Computer simulation of microstructures evolution for three-high cross-rolling of hollow steels[C]//2010 International Conference On Computer Design and Applications. Qinhuangdao:Institute of Electrical and Electronics Engineers,2010:V4-164. [35] ZHAO Yu-qian,YU En-lin,YAN Tao. Numerical simulation of deformation and microstructures evolution for hexagon hollow steels rolling[C]//2009 IEEE International Conference on Automation and Logistics. Shenyang:Institute of Electrical and Electronics Engineers, 2009:1672. [36] 郭锦,史佳新,陈雨来. 快速冷却前停留时间对微合金钢相变的作用[J]. 钢铁,2018,53(5):62.(GUO Jin,SHI Jia-xin,CHEN Yu-lai. Effect of delay time before rapid cooling on transformation of micro-alloyed steel[J]. Iron and Steel,2018,53(5):62.) [37] YU Wei,XIE Bao-sheng,WANG Ban,et al. Effect of rolling process on microstructure and properties of 95CrMo drill steel[J]. Journal of Iron and Steel Research,International,2016,23(9):910. [38] Fard R A,Kazeminezhad M. Effect of electropulsing on microstructure and hardness of cold-rolled low carbon steel[J]. Journal of Materials Research and Technology,2019,8(3):3114. [39] ZHANG Lin,HOU Yu-huang,GUO Xiao,et al. Effect of electromagnetic stirring on the microstructure and properties of Fe-Cr-Co steel[J]. Materials,2018,11(8):1437. [40] Deldar S,Mirzadeh H,Parsa M H. Prevention of surface hot shortness,development of banded structure,and mechanical properties of hot rolled Cu-bearing steel[J]. Engineering Failure Analysis,2016,68:132. [41] 朱洪武,刘雅政,徐盛,等. 退火工艺对钎具用钢22Si2Mn-CrNi2MoA带状组织的影响[J]. 北京科技大学学报,2013,35(3):312.(ZHU Hong-wu,LIU Ya-zheng,XU Sheng. Influence of annealing on the banded structure of 22Si2MnCr-Ni2MoA drill steel[J]. Journal of University of Science and Technology Beijing,2013,35(3):312.) [42] 纪元,闵云峰,李鹏善,等. 钢中带状组织及其研究现状[J]. 中国冶金,2016,26(4):1.(JI Yuan,MIN Yun-feng,LI Peng-shan,et al. Research status of banding phenomena in steels[J]. China Metallurgy,2016,26(4):1.) [43] 梁益龙,梁迟英,梁宇. 脉冲电流辅助热处理对EA4T车轴钢带状组织的影响[J]. 材料热处理学报,2011,32(10):62.(LIANG Yi-long,LIANG Chi-ying,LIANG Yu. Effect of electropulsing-aided heat treatment on band structure of EA4T axle steel[J]. Transactions of Materials and Heat Treatment,2011,32(10):62.) [44] 张国榉. 试论我国中空钎钢的几何结构参数[J]. 凿岩机械气动工具,2004(2):6.(ZHANG Guo-ju. Discussion of the geometrical structure parameters of hollow steel in China[J]. Rock Drilling Machines and Pneumatic Tools,2004(2):6.) [45] 姜杰凤. 奇数边中空钎钢成型过程的数值模拟[D]. 秦皇岛:燕山大学,2007.(JIANG Jie-feng. Numerical Simulation of Odd Number Hollow Drill steel[D]. Qinhuangdao:Yanshan University,2007.) [46] 许小林. 中空钢轧制过程数值模拟及尺寸精度分析[D]. 秦皇岛:燕山大学,2010.(XU Xiao-lin. Numerical Simulation and Analysis of Dimensional Accaracy of Hollow Drill Steel Rolling[D]. Qinhuangdao:Yanshan University,2010.) [47] 余伟,熊家泽,雷力齐,等. 轧制同轴复合棒材的芯材变形规律[J]. 钢铁研究学报,2016,28(8):33.(YU Wei,XIONG Jia-ze,LEI Li-qi,et al. Core rod deformation principle of rolled coaxial composite bar[J]. Journal of Iron and Steel Research,2016,28(8):33.) [48] 杨云,胡如好,李永金. 国内主要制钎企业的锥形钎对比分析[J]. 凿岩机械气动工具,2017(4):50.(YANG Yun,HU Ru-hao,LI Yong-jin. Comparison and analysis of tapered drilling rods from leading domestic drilling rods enterprises[J]. Rock Drilling Machines and Pneumatic Tools,2017(4):50.) [49] YAN Tao,QIN Na. Deformation analysis of asymmetric break-down rolling of hollow steel[J]. World Journal of Engineering,2017,14(6):483. [50] 吕庆功,牟仁玲,许文婧. 无缝钢管斜轧穿孔毛管壁厚偏心分析[J]. 钢铁,2017,52(8):65.(LÜ Qing-gong,MU Ren-ling,XU Wen-jing. Analysis on wall thickness eccentricity of cross-roll pierced shells of seamless steel tube[J]. Iron and Steel,2017,52(8):65.) [51] 康永林,朱国明,陶功明,等. 高精度型钢轧制数字化技术及应用[J]. 钢铁,2017,52(3):49.(KANG Yong-lin,ZHU Guo-ming,TAO Gong-ming,et al. Digital technology and application of high precision section steel rolling[J]. Iron and Steel,2017,52(3):49.) [52] ZHAO Yu-qian,YU En-lin,YAN Tao. Deformation analysis of seamless steel tube in cross rolling piercing process[C]//2010 International Conference On Computer Design and Applications. Qinhuangdao:Institute of Electrical and Electronics Engineers,2010:V3-320. [53] 杨庚朝,杨俊,刘建. 高等级钎具中空钢ZK55SiMnMo产品开发[J]. 金属材料与冶金工程,2018,46(5):3.(YANG Geng-chao,YANG Jun,LIU Jian. Development of high grade hollow drill steel ZK55SiMnMo[J]. Metal Materials and Metallurgy Engineering,2018,46(5):3.) [54] 白振华,徐纪栓,董航哲,等. 平整轧制过程中工作辊粗糙度衰减模型[J]. 钢铁,2019,54(4):43.(BAI Zhen-hua,XU Ji-shuan,DONG Hang-zhe,et al. Roller roughness attenuation model in leveling rolling process[J]. Iron and Steel,2019,54(4):43.) [55] 尚飞,李洪波,张杰,等. CVC工作辊非对称磨损分析与预报模型建立[J]. 钢铁,2016,51(6):59.(SHANG Fei,LI Hong-bo,ZHANG Jie,et al. Asymmetric wear and wear prediction model of CVC work roll[J]. Iron and Steel,2016,51(6):59.) [56] 刘世华. 用局部应力-应变法估算钎杆寿命[J]. 凿岩机械气动工具,2000(1):24.(LIU Shi-hua. Estimate the drill rod life by local stress-strain[J]. Rock Drilling Machines and Pneumatic Tools,2000(1):24.) [57] 赵景芳,马龙才,宋林松,等. 国外钻杆疲劳寿命预测系统模型及应用[J]. 石油机械,2016,44(12):1.(ZHAO Jing-fang,MA Long-cai,SONG Lin-song,et al. The foreign drill pipe fatigue life prediction model and its application[J]. China Petroleum Machinery,2016,44(12):1.) [58] Hosoi A,Kishi T,Ju Y. Healing of fatigue crack by high-density electropulsing in austenitic stainless steel treated with the surface-activated pre-coating[J]. Materials,2013,6(9):4213.