Revamping of Bar Production Line for Ultra Fine Grained Ribbed Bars |
ZHANG Hai1, 2,TONG Jinping3,LIANG Yuncai4, ZHANG Enmin5,YANG Fan5 |
1. Materials Science and Engineering Institute, University of Science and Technology Beijing, Beijing 100083, China;2. Tangshan Iron and Steel Group, Tangshan 063000, Hebei,China; 3. Continuous Rolling Middle Section Plant Xuanhua Iron and Steel Group Co., of Tangshan Iron and Steel Group, Xuanhua 075100, Hebei, China;4. First Small Section Rolling Mill Of Jin’an Iron and Steel Group Co. , Jin’an 250101,Shandong, China;5. Beijing Adler Bauwerk Engineering and Technology Co., Ltd., Beijing 100086, China |
|
|
Abstract The production line was revamped with addition of water cooling devices between roughing and intermediate trains and after finishing tain and a control system for adjustment of water flow rate, water temperature, water pressure, rolling piece temperature and position.The results show,that for ribbed bars of 20MnSi and 20MnSiNb 475m3/h of water flow rate, 1.5MPa of water pressure, 14.5m/s of rolling speed are suitable.
|
Received: 01 January 1900
|
|
|
|
[1] |
. [J]. , 2019, 44(3): 0-0. |
[2] |
HE Tian-ren. Analysis and Application of Interstand Cooling Technology for Plate Rolling[J]. Iron and Steel, 2013, 48(12): 57-62. |
[3] |
. High-Precision Temperature Model for Plant Cooling Process[J]. Chinese Journal of Iron and Steel, 2010, 22(08): 27-27. |
[4] |
CUI Qingling;ZHAO Min;YUAN Guo;LIU Xianghua;WANG Guodong. Numerical Simulation of Steel Plate Runout Table Cooling and Its Deformation Analysis[J]. Chinese Journal of Iron and Steel, 2007, 19(9): 21-0. |
[5] |
LI Guiyang;MA Liming;ZHANG Zhiqiang;FENG Jianhang;LI Jiazheng. Production Practice of 20MnSiNb HRB400 Rebar[J]. Iron and Steel, 2006, 41(5): 0-0. |
|
|
|
|