摘要

低碳铝镇静钢铸坯皮下有明显的钩状坯壳,钩状坯壳很容易捕获夹杂物和气泡,使得簇群状氧化铝夹杂和气泡+氧化铝在铸坯的近表层聚集。对低碳铝镇静钢铸坯的宽面、窄面以及角部综合取样,研究分析了铸坯不同位置处钩状坯壳的特征与变化规律。结果显示,在铸坯宽面,中心处钩状坯壳较深;在铸坯窄面,越靠近角部,钩状坯壳越深;在铸坯角部,钩状坯壳呈现三维形貌。此外,提出了钩状坯壳对夹杂物和气泡的捕获机理,认为连铸过程中的Marangoni力对夹杂物和气泡的捕获起着至关重要的作用。此机理很好地解释了钩状坯壳更易捕获大尺寸夹杂物和气泡的原因;根据该机理,提出了减小钩状坯壳捕获大尺寸夹杂物的相关措施。

Abstract

A distinctive microstructural feature called a “hook” is often observed on the subsurface of low carbon aluminum- killed steel slabs during continuous casting processes. Inclusions and bubbles are easy to be entrapped by the hooks,which makes Al2O3 cluster and “Ar+Al2O3” type inclusions gathered in subsurface layer of the slabs. A large number of samples were obtained from wide face,narrow face,and corner of the slab in this experiment. The characteristics of hooks in different positions of the slab were investigated. The results showed that in the wide face the center of hooks are deeper than others,in the narrow face the hook depth increase when close to the corner of slab,and hooks near the corners of the slab exhibited three- dimensional morphology. Furthermore,a mechanism of hooks entrapping alumina inclusions and argon bubbles was proposed,which suggested that marangoni force in the process of continuous casting plays an important role on the entrapment of alumina inclusions and argon bubbles. By investigating the behavior of inclusions and bubbles in solidification front of hooks,this mechanism explained the process of how hooks entrapping large side inclusions and bubbles well. From the result,the countermeasure of reduction of hooks and inclusions was proposed.

关键词

连铸 / 钩状坯壳 / 低碳铝镇静钢 / 非金属夹杂物 / 气泡 / 表面张力梯度

图表

引用本文

导出引用
苑鹏, 邓小旋, 姜敏, . 低碳铝镇静钢铸坯皮下钩状坯壳[J]. 钢铁, 2015, 50(8): 24-33 https://doi.org/10.13228/j.boyuan.issn0449-749x.20140589
YUN Peng, DENG Xiao-Xuan, JIANG Min, et al. Investigation of subsurface hooks in continuous cast low carbon aluminum- killed steel slab[J]. Iron and Steel, 2015, 50(8): 24-33 https://doi.org/10.13228/j.boyuan.issn0449-749x.20140589
中图分类号: TF777.1   

参考文献

[1]Awajiya Y, Kubota Y, Takeuchi S.Inclusion Entrapment Location in Solidified Shell of Ultra Low Carbon Steel Slab[C] // AISTech Proceedings Charlotte, NC; USA, 2005: 65. [2]Mizukami H, Hiraki S, Kawamoto M, et al.Initial Solidification Behavior of Ultra-low,Low and Middle Carbon Steel[J].ISIJ International, 1999, 39(12):1262- [3]Takeuchi E, Brimacombe J K.The Formation of Oscillation Marks in the Continuous Casting of Steel Slabs[J].Metallurgical and Materials Transactions B, 1984, 15(3):493- [4]Brimacombe J K, Sorimachi K.Crack Formation in the Continuous Casting of Steel[J].Metallurgical and Materials Transactions B, 1977, 8(2):489- [5]Takeuchi E, Brimacombe J K.Effect of Oscillation-mark Formation on the Surface Quality of Continuously Cast Steel Slabs[J].Metallurgical and materials transactions B, 1985, 16(3):605- [6]Sengupta J, Shin H J, Thomas B G, et al.Micrograph Evidence of Meniscus Solidification and Sub-surface Microstructure Evolution in Continuous-cast Ultralow-carbon Steels[J].Acta Materialia, 2006, 54(4):1165- [7]Schmidt K D, Friedel F, Imlau K, Jager W, Muller KT.Consequent Improvement of Surface Quality by Systematic Analysis of Slabs[J].[J].Steel Research International, 2003, (74):659- [8]Birat J-P, Larrecq M, Lamant J-Y, PetegiefJ.The Continuous Casting Mold: A Basic Tool for Surface Quality and Strand Productivity[J], [J].Steelmaking Conference Proceedings, 1991, (74):39- [9]Shin H J, Thomas B G, Lee G G, et al.Analysis of Hook Formation Mechanism in Ultra Low Carbon Steel using CON1D Heat Flow-Solidification Model[J][J].Materials Science & Technology,, 2004, :11- [10]Sengupta J, Thomas B G, Shin H J, et al.A New Mechanism of Hook Formation during Continuous Casting of Ultra-low-carbon Steel Slabs[J].Metallurgical and Materials Transactions A, 2006, 37(5):1597- [11]Sengupta J, Thomas B G, Shin H, et al.Mechanism of Hook Formation in Ultralow-carbon Steel Based on Microscopy Analysis and Thermalstress Modeling[J].Iron and Steel Technology, 2007, 4(7):83- [12]Lee G G, Thomas B G, Kim S H, et al.Microstructure Near Corners of Continuous-cast Steel Slabs Showing Three-dimensional Frozen Meniscus and Hooks[J].Acta Materialia, 2007, 55(20):6705- [13]杨文, 许志刚, 薛勇强, 等.钢连铸头坯亚表层 结构特征[J].北京科技大学学报, 2012, 33(11):1341- [14]Yamamura H, Mizukami Y, Misawa K.Formation of a Solidified Hook-like Structure at the Subsurface in Ultra Low Carbon Steel[J].ISIJ International, 1996, 36(Suppl):S223- [15]Deng X-X, Li L-P, Wang X-H, et al.Subsurface Macro-Inclusions and Solidified Hook Character in Aluminum-Killed Deep-Drawing Steel Slabs[J].International Journal of Minerals, Metallurgy and Materials, 2014, 21(6):531- [16]Wang Z, Mukai K, Lee I J.Behavior of Fine Bubbles in Front of the Solidifying Interface[J].ISIJ International, 1999, 39(6):553- [17]Lee S M, Kim S J, Kang Y B, et al.Numerical Analysis of Surface Tension Gradient Effect on the Behavior of Gas Bubbles at the SolidLiquid Interface of Steel[J].ISIJ International, 2012, 52(10):1730- [18]Mukai K, Lin W.Behavior of Non-metallic Inclusions and Bubbles in Front of Solidifying Interface of Liquid Iron[J].Tetsu-to-Hagan, 1994, 80(7):533- [19]Mukai K, Zeze M.Motion of Fine Particles under Interfacial Tension Gradient in Relation to Continuous Casting Process[J].Steel Research International, 2003, 74(3):131- [20]Matsushita T, Mukai K, Zeze M.Correspondence between Surface Tension Estimated by a Surface Thermodynamic Model and Number of Bubbles in the Vicinity of the Surface of Steel Products in Continuous Casting Process[J].ISIJ International, 2013, 53(1):18- [21]Miyake T, Morishita M, Nakata H, et al.Influence of Sulphur Content and Molten Steel Flow on Entrapment of Bubbles to SolidLiquid Interface[J].ISIJ international, 2006, 46(12):1817- [22]Belton G R.Langmuir Adsorption,the Gibbs Adsorption Isotherm,and Interracial Kinetics in Liquid Metal Systems[J].Metallurgical and Materials Transactions B, 1976, 7(1):35- [23]Sahoo P, DebRoy T, McNallan M J.Surface Tension of Binary Metal—Surface Active Solute Systems under Conditions Relevant to Welding Metallurgy[J].Metallurgical and Materials Transactions B, 1988, 19(3):483- [24]Mukai K, Lin W.Motion of Small Particles in Solution with a Interfacial Tension Gradient and Engulfment of the Particles by Solidifying Interface[J].Tetsu-to-Hagan, 1994, 80(7):527- [25]Lee G G, Shin H J, Kim S H, et al.Prediction and Control of Subsurface Hooks in Continuous Cast Ultra-low-carbon Steel Slabs[J].Ironmaking & Steelmaking, 2009, 36(1):39-

7

Accesses

0

Citation

Detail

段落导航
相关文章

/