降低钢中全氧含量的精炼工艺技术

  • 张敏
作者信息 +

Refining Technology for Reducing w([TO]) in Steel

  • 张敏
Author information +
文章历史 +

摘要

为实现高品质低氧钢的生产,有效降低钢中全氧含量,在考虑转炉下渣、炉渣氧化性以及钢水氧活度影响的前提下,通过研究钢包渣改质技术、过程钢包渣氧化性控制技术以及相应的钢包底吹氩制度等精炼工艺,建立了转炉-连铸流程生产低氧钢的精炼工艺技术。采用该技术生产的高品质优特钢成品w([TO])≤15×10-6。

Abstract

In order to produce low oxygen steel with high quality, converter slag-tapping, slag oxidability and oxygen activity were analyzed. In addition, modifying and adding process of slag, control of slag oxidability and bottom argon-blowing in ladle were researched as well. On this basis, refining process which is good for low oxygen steel producing with converter-continuous casting process has been developed. The results show that w([TO]) in steel is not more than 15×10-6.

关键词

低氧钢 / 夹杂物 / T[O] / 精炼

Key words

low oxygen steel / inclusions / T[O] / refining

图表

引用本文

导出引用
张敏. 降低钢中全氧含量的精炼工艺技术[J]. 钢铁, 2011, 46(7): 41-44
ZHANG Min. Refining Technology for Reducing w([TO]) in Steel[J]. Iron and Steel, 2011, 46(7): 41-44

Accesses

Citation

Detail

段落导航
相关文章

/