某4060m3高炉炉缸破损调查
Investigation on carbon brick erosion in the hearth of a 4060m3 BF
-
摘要: 对某4060 m3高炉炉缸破损状况进行调查,分析炉缸炭砖侵蚀状况,并从化学成分及微观结构等方面讨论了炭砖侵蚀的原因。结果表明:(1)铁口中心线以下区域炭砖侵蚀最严重,且周向分布不均,1号铁口对应区域侵蚀最为显著,炉底炭砖保存完好,炉缸炭砖侵蚀总体呈“蒜头状”;(2)进一步对侵蚀严重区域取样调查发现,炭砖存在分层现象,炭砖热面无渣皮保护,砖缝中有锌沉积物;(3)锌与碱金属渗透是炭砖脆化层形成的主要原因,锌发挥主导作用,铁水化学侵蚀、热应力引发的环裂及有害元素渗透是炉缸炭砖侵蚀的原因。Abstract: This study analyzes the erosion of hearth carbon bricks in a domestic 4000m3 blast furnace after investigation,and analyzes the reason of carbon brick erosion from chemical composition and microstructure aspect.The results show that(1) the carbon bricks is eroded unevenly in height and circumferential direction,the most severe erosion occurs in the area below the centerline of the taphole,especially for No.1 taphole of the furnace,of which the carbon bricks at the bottom remain intact,while the carbon brick erosion of the hearth exhibits a "garlic bulb" shape;(2) further investigation by sampling severely eroded areas shows that stratification occurs in carbon bricks there,the hot surface of the carbon bricks is not protected with slag skull any longer,and zinc is found deposited in the brick joints;(3) the penetration of zinc and base metals is regarded as the primary cause of carbon brick stratification with zinc as a dominant factor,while hearth carbon brick erosion is resulted from circumferential cracking induced by hot metal chemical corrosion and thermal stress,and penetration of harmful elements.
下载: