投审稿入口

柳钢2号高炉镁铝比调控及稳定顺行措施

Countermeasures for regulation of(MgO)/(Al2O3) ratio and stable smooth running of No.2 BF in Liuzhou Steel

  • 摘要: 针对高炉降本与稳定运行的矛盾,对柳钢2号高炉进行镁铝比调控,逐步将烧结矿MgO由2.1%下调至1.8%,炉渣(MgO)由8.65%降至7.28%,镁铝比由0.55降至0.44。调整后,炉渣黏度上升,脱硫能力下降,为维持高炉稳定顺行,采取了相应措施,包括:改善烧结矿质量并优化炉料结构,控制炉温及渣铁成分,调整送风制度及装料制度,优化炉前出铁作业等。通过采取以上措施,镁铝比下调后高炉实现稳定顺行,利用系数上升0.332t/(m3·d),燃料比稳定在520kg/t左右,煤比大幅度提升25kg/t,主要经济技术指标表现良好。

     

    Abstract: Facing the contradictory goals of cost reduction and stable running,Liuzhou Steel exercises a regulation of(MgO)/(Al2O3) ratio in its No.2 BF with MgO content in sinter reduced gradually from 2.1% to 1.8%,the(MgO) content in slag decreased from 8.65% to 7.28%,and the(MgO)/(Al2O3) ratio reduced from 0.55 to 0.44.Subsequently,the slag viscosity increases,and the desulfurization capacity weakens.To maintain smooth running of the furnace,corresponding countermeasures are implemented,including improving sinter quality,optimizing the burden mix and controlling furnace temperature and slag/iron comp osition.In addition,the operator also adjusts the blasting and charging systems,and optimizes the tapping operations.These efforts result in stable and smooth running of the furnace after lowering the(MgO)/(Al2O3) ratio;the productivity posts 0.332t/(m3·d) rise,the fuel rate stabilizes at about 520kg/t and the pulverized coal injection rate surges by 25 kg/t,indicating favorable main techno-economic indicators.

     

/

返回文章
返回