投审稿入口

西昌钢钒1号高炉高比例钒钛球团矿冶炼工业试验

Industrial test of Xichang Steel & Vanadium No.1 BF smelting with high-proportion V-Ti pellet

  • 摘要: 西昌钢钒高炉长期以钒钛烧结矿为主要原料,但钒钛烧结矿冶金性能差,影响炉况顺行,为此在1号高炉开展高比例钒钛球团矿冶炼工业试验。随着钒钛球团矿配比的提高,炉料性能出现以下变化:(1)钒钛烧结矿转鼓指数提高;(2)炉料体积密度上升、自然堆角减小,软化开始温度、软化终了温度升高,软化区间变宽,熔化开始温度升高,滴落温度降低,熔滴区间变窄,熔滴性能改善。高比例钒钛球团矿冶炼条件下,通过优化操作制度,高炉焦比从439.42 kg/t降至413.08kg/t,燃料比降低5.94kg/t,利用系数从2.468t/(m3·d)提高至2.700t/(m3·d)。

     

    Abstract: Xichang Steel and Vanadium takes vanadium-titanium sinter as the main raw material for its blast furnace for a long time,but the poor metallurgical property of vanadium-titanium sinter affects the smooth running of the furnace.For this reason,an industrial test is carried out in its No.1 BF by using high proportion of vanadium-titanium pellets,and following variation appears in the burden physical property and softening-melting behavior as the proportion of vanadium-titanium pellets increase s:(1) the tumbler index of vanadium-titanium sinter improves;(2) the bulk density of the burden increases,the natural repose angle decreases,the softening start and end temperature rises,the softening temperature range widens,the melting start temperature increases,the dripping temperature falls,the difference between melting start temperature and dripping start temperature narrows,and the soft-melt dripping behavior improves.Under the smelting condition of high proportion of vanadium-titanium pellets,optimization in operating system makes the coke rate of the blast furnace dropping from439.42 kg/t to 413.08 kg/t,the fuel rate lowered by 5.94kg/t,and the BF productivity improved from 2.468t/(m3·d) to2.700t/(m3·d).

     

/

返回文章
返回